DISPLAY DEVICE WITH THIN-FILM METAL-ORGANIC MIXED LAYER HAVING REDUCED REFLECTANCE

PROBLEM TO BE SOLVED: To provide a display device having a thin metal-organic mixed layer (MOML) that contains a metal (contained material) and an organic material and has a thickness less than 175 nm. SOLUTION: The thin metal-organic mixed layer may be of a single or multilayer configuration. The r...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HONEY AJIZU, NEMANJA STEFANOVIC, POPOVIC ZORAN D, COGGAN JENNIFER A
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a display device having a thin metal-organic mixed layer (MOML) that contains a metal (contained material) and an organic material and has a thickness less than 175 nm. SOLUTION: The thin metal-organic mixed layer may be of a single or multilayer configuration. The reflectance (%) of the device can be controlled by varying the thickness of the MOML, the metal components and the concentrations of the metal components in the MOML. COPYRIGHT: (C)2007,JPO&INPIT