METHOD FOR PREVENTING CLOGGING OF NOZZLE IN CONTINUOUS CASTING FOR STEEL

PROBLEM TO BE SOLVED: To provide a method for achieving a stable continuous casting operation without clogging a ladle nozzle and an immersion nozzle. SOLUTION: A method for preventing the clogging of the nozzle, is performed as the followings, by which FeSi, FeMn, FeP, FeCr alloys are added into mo...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MATSUBA SHIGEKAZU, NAKAJIMA HIROYOSHI, YAMAGUCHI JUN, WATANABE YU, MIZOGUCHI TOSHIAKI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a method for achieving a stable continuous casting operation without clogging a ladle nozzle and an immersion nozzle. SOLUTION: A method for preventing the clogging of the nozzle, is performed as the followings, by which FeSi, FeMn, FeP, FeCr alloys are added into molten steel exceeding 50 ppm soluble oxygen concentration so as to become ≥80% of the aimed concentration shown with mass% in each element to the aimed Si, Mn, P, Cr concentrations in a molten steel in a tundish or a cast slab. Further, the method for preventing the clogging of the nozzle, is performed as the followings, in which total Ca mixed quantity from these alloys is limited so that the charging quantity of the added FeSi, FeMn, FeP, FeCr alloys satisfies the following formula (A) after Al-deoxidation. That is, the above (A) formula is Total Ca mixed quantity=(0.5×WFeSi×CaFeSi/100+0.01×WFeMn×CaFeMn/100+0.02×WFeP×CaFeP/100+0.005×WFeCr×CaFeCr/100)/Wsteel×106≤6. Wherein, Wi(kg) is added quantity of i alloy after Al deoxidation, Wsteel(kg) is molten steel quantity and Cai(mass%) is Ca concentration in the ferro-alloy i. COPYRIGHT: (C)2006,JPO&NCIPI