BLOWN ASPHALT FOR WATERPROOFING WORK AND METHOD FOR PRODUCING THE SAME
PROBLEM TO BE SOLVED: To provide blown asphalt pertinent to waterproofing work excellent in workability and storability, by suppressing odor and smoke arising at heating and melting the blown asphalt for waterproofing work at a high temperature. SOLUTION: This blown asphalt for waterproofing work is...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide blown asphalt pertinent to waterproofing work excellent in workability and storability, by suppressing odor and smoke arising at heating and melting the blown asphalt for waterproofing work at a high temperature. SOLUTION: This blown asphalt for waterproofing work is characterized by having a softening point of 100-120°C, a needle penetration degree of 25-35, oil exudation of ≤3, folding resistance at a low temperature of ≤1°C, a temperature at which viscosity becomes 100 mPa×s of ≤220°C, and a temperature at which viscosity becomes 60 mPa×s of ≤240°C. COPYRIGHT: (C)2006,JPO&NCIPI |
---|