METHOD FOR PRODUCING HIGH CARBON CHROMIUM BEARING STEEL
PROBLEM TO BE SOLVED: To provide a technique capable of highly suppressing huge carbides in spite of short time soaking. SOLUTION: In the method, a slab for high carbon chromium bearing steel is at least subjected to soaking and hot rolling, thus high carbon chromium bearing steel is produced. Also,...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide a technique capable of highly suppressing huge carbides in spite of short time soaking. SOLUTION: In the method, a slab for high carbon chromium bearing steel is at least subjected to soaking and hot rolling, thus high carbon chromium bearing steel is produced. Also, in the method where the soaking temperature of 1,150 to 1,260°C is adopted, as the slab for high carbon chromium bearing steel, the one having a P concentration of 0.002 to 0.009 mass% is used, and the holding time of the soaking temperature is controlled to |
---|