METHOD FOR PRODUCING CARBON BLACK DISPERSED POLYAMIC ACID SOLUTION AND SEMICONDUCTIVE POLYIMIDE BELT

PROBLEM TO BE SOLVED: To provide a method for producing a polyamic acid solution in which carbon black is prevented from aggregation and dispersed in a stabilized particle size, and to provide a semiconductive polyimide belt by using the solution. SOLUTION: The method for producing the carbon black...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WATANABE YOSHINOBU, KAMIBAYASHI MASAHIRO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a method for producing a polyamic acid solution in which carbon black is prevented from aggregation and dispersed in a stabilized particle size, and to provide a semiconductive polyimide belt by using the solution. SOLUTION: The method for producing the carbon black dispersed polyamic acid solution is characterized as follows: in a method for producing a carbon black dispersed polyamic acid solution comprising the steps of dissolving a tetracarboxylic dianhydride component and a diamine component in a dispersion containing carbon black dispersed therein and polymerizing the resulting mixture, a step of kneading the polyamic acid solution under a shear stress of 0.0001-1 MPa is introduced into after the polymerization step. There are also provided the carbon black dispersed polyamic acid solution obtained by the production method and the semiconductive polyimide belt yielded by using the carbon black dispersed polyamic acid solution. COPYRIGHT: (C)2005,JPO&NCIPI