METHOD FOR FORMING OPTICAL FIBER
PROBLEM TO BE SOLVED: To reduce attenuation of a glass optical fiber due to heat aging and Rayleigh scattering in a heat treatment of the fiber. SOLUTION: In the method for forming an optical fiber, the optical fiber is formed by drawing at ≥10 m/sec draw rate from a heated glass source (block 10) a...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To reduce attenuation of a glass optical fiber due to heat aging and Rayleigh scattering in a heat treatment of the fiber. SOLUTION: In the method for forming an optical fiber, the optical fiber is formed by drawing at ≥10 m/sec draw rate from a heated glass source (block 10) and is heat-treated by maintaining the optical fiber within a heated treatment zone for the total resident time of 0.07-0.25 sec, while subjecting the optical fiber to an average cooling rate of 1,200-5,000 °C/sec defined by ä[fiber surface temperature in an inlet zone]-[fiber surface temperature in the outlet zone]}/[the total resident time of the optical fiber in the treatment zone] (block 20). COPYRIGHT: (C)2005,JPO&NCIPI |
---|