POLYESTER AND BLOW MOLDED ARTICLE MADE THEREFROM
PROBLEM TO BE SOLVED: To obtain a polyester resin generating little acetaldehyde in the molding of a preform or a bottle. SOLUTION: The polyester is formed from terephthalic acid and/or isophthalic acid and ethylene glycol. It has an intrinsic viscosity of ≥0.60 [dl/g] and a density of ≥1,390 kg/m3a...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To obtain a polyester resin generating little acetaldehyde in the molding of a preform or a bottle. SOLUTION: The polyester is formed from terephthalic acid and/or isophthalic acid and ethylene glycol. It has an intrinsic viscosity of ≥0.60 [dl/g] and a density of ≥1,390 kg/m3and satisfies the formula 1: (AA4h-AA1h)≤1.0 ppm wherein AA1his the weight ratio of AA (acetaldehyde) extracted in hot water under the condition of 120°C×1hr and AA4his the weight ratio of AA extracted in hot water under the condition of 120°C×4hr. COPYRIGHT: (C)2005,JPO&NCIPI |
---|