POWDER FOR MAGNETIC CORE, POWDER-COMPACTED MAGNETIC CORE, AND THEIR PRODUCTION METHOD

PROBLEM TO BE SOLVED: To provide a powder-compacted magnetic core having high magnetic flux density and low loss. SOLUTION: The powder-compacted magnetic core is obtained by compacting powder for a magnetic core composed of magnetic powder essentially consisting of Fe and Si and an insulated film fo...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: CHOU KOKUHOU, SUGIYAMA MASAKI, HIGASHIYAMA KIYOSHI, KIKKO TADAYOSHI, KONDO MIKIO, HATTORI TAKESHI, TAJIMA SHIN, KISHIMOTO HIDESHI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator CHOU KOKUHOU
SUGIYAMA MASAKI
HIGASHIYAMA KIYOSHI
KIKKO TADAYOSHI
KONDO MIKIO
HATTORI TAKESHI
TAJIMA SHIN
KISHIMOTO HIDESHI
description PROBLEM TO BE SOLVED: To provide a powder-compacted magnetic core having high magnetic flux density and low loss. SOLUTION: The powder-compacted magnetic core is obtained by compacting powder for a magnetic core composed of magnetic powder essentially consisting of Fe and Si and an insulated film formed on the surfaces of the particles of the magnetic powder. The insulated film is obtained by subjecting the magnetic powder to external oxidation treatment. The specific oxygen content (g/m2) denoting the oxygen content (g) per unit surface area (m2) of the magnetic powder is 0.005 to 0.05 g/m2. Since the insulated film is thin and has excellent heat resistance, at the time when the magnetic powder coated with the insulated film is used, the powder-compacted magnetic core having high magnetic flux density and low hysteresis loss can be obtained. COPYRIGHT: (C)2005,JPO&NCIPI
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2005146315A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2005146315A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2005146315A3</originalsourceid><addsrcrecordid>eNrjZAgN8A93cQ1ScPMPUvB1dPdzDfF0VnD2D3LVUYDI6Dr7-wY4Ooe4uqDLO_q5KIR4uHoGKQQE-buEOod4-vsp-LqGePi78DCwpiXmFKfyQmluBiU31xBnD93Ugvz41OKCxOTUvNSSeK8AIwMDU0MTM2NDU0djohQBAJCEMH0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>POWDER FOR MAGNETIC CORE, POWDER-COMPACTED MAGNETIC CORE, AND THEIR PRODUCTION METHOD</title><source>esp@cenet</source><creator>CHOU KOKUHOU ; SUGIYAMA MASAKI ; HIGASHIYAMA KIYOSHI ; KIKKO TADAYOSHI ; KONDO MIKIO ; HATTORI TAKESHI ; TAJIMA SHIN ; KISHIMOTO HIDESHI</creator><creatorcontrib>CHOU KOKUHOU ; SUGIYAMA MASAKI ; HIGASHIYAMA KIYOSHI ; KIKKO TADAYOSHI ; KONDO MIKIO ; HATTORI TAKESHI ; TAJIMA SHIN ; KISHIMOTO HIDESHI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a powder-compacted magnetic core having high magnetic flux density and low loss. SOLUTION: The powder-compacted magnetic core is obtained by compacting powder for a magnetic core composed of magnetic powder essentially consisting of Fe and Si and an insulated film formed on the surfaces of the particles of the magnetic powder. The insulated film is obtained by subjecting the magnetic powder to external oxidation treatment. The specific oxygen content (g/m2) denoting the oxygen content (g) per unit surface area (m2) of the magnetic powder is 0.005 to 0.05 g/m2. Since the insulated film is thin and has excellent heat resistance, at the time when the magnetic powder coated with the insulated film is used, the powder-compacted magnetic core having high magnetic flux density and low hysteresis loss can be obtained. COPYRIGHT: (C)2005,JPO&amp;NCIPI</description><edition>7</edition><language>eng</language><subject>ALLOYS ; BASIC ELECTRIC ELEMENTS ; CASTING ; CHEMISTRY ; ELECTRICITY ; FERROUS OR NON-FERROUS ALLOYS ; INDUCTANCES ; MAGNETS ; MAKING METALLIC POWDER ; MANUFACTURE OF ARTICLES FROM METALLIC POWDER ; METALLURGY ; PERFORMING OPERATIONS ; POWDER METALLURGY ; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES ; TRANSFORMERS ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS ; WORKING METALLIC POWDER</subject><creationdate>2005</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20050609&amp;DB=EPODOC&amp;CC=JP&amp;NR=2005146315A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20050609&amp;DB=EPODOC&amp;CC=JP&amp;NR=2005146315A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>CHOU KOKUHOU</creatorcontrib><creatorcontrib>SUGIYAMA MASAKI</creatorcontrib><creatorcontrib>HIGASHIYAMA KIYOSHI</creatorcontrib><creatorcontrib>KIKKO TADAYOSHI</creatorcontrib><creatorcontrib>KONDO MIKIO</creatorcontrib><creatorcontrib>HATTORI TAKESHI</creatorcontrib><creatorcontrib>TAJIMA SHIN</creatorcontrib><creatorcontrib>KISHIMOTO HIDESHI</creatorcontrib><title>POWDER FOR MAGNETIC CORE, POWDER-COMPACTED MAGNETIC CORE, AND THEIR PRODUCTION METHOD</title><description>PROBLEM TO BE SOLVED: To provide a powder-compacted magnetic core having high magnetic flux density and low loss. SOLUTION: The powder-compacted magnetic core is obtained by compacting powder for a magnetic core composed of magnetic powder essentially consisting of Fe and Si and an insulated film formed on the surfaces of the particles of the magnetic powder. The insulated film is obtained by subjecting the magnetic powder to external oxidation treatment. The specific oxygen content (g/m2) denoting the oxygen content (g) per unit surface area (m2) of the magnetic powder is 0.005 to 0.05 g/m2. Since the insulated film is thin and has excellent heat resistance, at the time when the magnetic powder coated with the insulated film is used, the powder-compacted magnetic core having high magnetic flux density and low hysteresis loss can be obtained. COPYRIGHT: (C)2005,JPO&amp;NCIPI</description><subject>ALLOYS</subject><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CASTING</subject><subject>CHEMISTRY</subject><subject>ELECTRICITY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>INDUCTANCES</subject><subject>MAGNETS</subject><subject>MAKING METALLIC POWDER</subject><subject>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES</subject><subject>TRANSFORMERS</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><subject>WORKING METALLIC POWDER</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2005</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZAgN8A93cQ1ScPMPUvB1dPdzDfF0VnD2D3LVUYDI6Dr7-wY4Ooe4uqDLO_q5KIR4uHoGKQQE-buEOod4-vsp-LqGePi78DCwpiXmFKfyQmluBiU31xBnD93Ugvz41OKCxOTUvNSSeK8AIwMDU0MTM2NDU0djohQBAJCEMH0</recordid><startdate>20050609</startdate><enddate>20050609</enddate><creator>CHOU KOKUHOU</creator><creator>SUGIYAMA MASAKI</creator><creator>HIGASHIYAMA KIYOSHI</creator><creator>KIKKO TADAYOSHI</creator><creator>KONDO MIKIO</creator><creator>HATTORI TAKESHI</creator><creator>TAJIMA SHIN</creator><creator>KISHIMOTO HIDESHI</creator><scope>EVB</scope></search><sort><creationdate>20050609</creationdate><title>POWDER FOR MAGNETIC CORE, POWDER-COMPACTED MAGNETIC CORE, AND THEIR PRODUCTION METHOD</title><author>CHOU KOKUHOU ; SUGIYAMA MASAKI ; HIGASHIYAMA KIYOSHI ; KIKKO TADAYOSHI ; KONDO MIKIO ; HATTORI TAKESHI ; TAJIMA SHIN ; KISHIMOTO HIDESHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2005146315A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2005</creationdate><topic>ALLOYS</topic><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CASTING</topic><topic>CHEMISTRY</topic><topic>ELECTRICITY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>INDUCTANCES</topic><topic>MAGNETS</topic><topic>MAKING METALLIC POWDER</topic><topic>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES</topic><topic>TRANSFORMERS</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><topic>WORKING METALLIC POWDER</topic><toplevel>online_resources</toplevel><creatorcontrib>CHOU KOKUHOU</creatorcontrib><creatorcontrib>SUGIYAMA MASAKI</creatorcontrib><creatorcontrib>HIGASHIYAMA KIYOSHI</creatorcontrib><creatorcontrib>KIKKO TADAYOSHI</creatorcontrib><creatorcontrib>KONDO MIKIO</creatorcontrib><creatorcontrib>HATTORI TAKESHI</creatorcontrib><creatorcontrib>TAJIMA SHIN</creatorcontrib><creatorcontrib>KISHIMOTO HIDESHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>CHOU KOKUHOU</au><au>SUGIYAMA MASAKI</au><au>HIGASHIYAMA KIYOSHI</au><au>KIKKO TADAYOSHI</au><au>KONDO MIKIO</au><au>HATTORI TAKESHI</au><au>TAJIMA SHIN</au><au>KISHIMOTO HIDESHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>POWDER FOR MAGNETIC CORE, POWDER-COMPACTED MAGNETIC CORE, AND THEIR PRODUCTION METHOD</title><date>2005-06-09</date><risdate>2005</risdate><abstract>PROBLEM TO BE SOLVED: To provide a powder-compacted magnetic core having high magnetic flux density and low loss. SOLUTION: The powder-compacted magnetic core is obtained by compacting powder for a magnetic core composed of magnetic powder essentially consisting of Fe and Si and an insulated film formed on the surfaces of the particles of the magnetic powder. The insulated film is obtained by subjecting the magnetic powder to external oxidation treatment. The specific oxygen content (g/m2) denoting the oxygen content (g) per unit surface area (m2) of the magnetic powder is 0.005 to 0.05 g/m2. Since the insulated film is thin and has excellent heat resistance, at the time when the magnetic powder coated with the insulated film is used, the powder-compacted magnetic core having high magnetic flux density and low hysteresis loss can be obtained. COPYRIGHT: (C)2005,JPO&amp;NCIPI</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2005146315A
source esp@cenet
subjects ALLOYS
BASIC ELECTRIC ELEMENTS
CASTING
CHEMISTRY
ELECTRICITY
FERROUS OR NON-FERROUS ALLOYS
INDUCTANCES
MAGNETS
MAKING METALLIC POWDER
MANUFACTURE OF ARTICLES FROM METALLIC POWDER
METALLURGY
PERFORMING OPERATIONS
POWDER METALLURGY
SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
TRANSFORMERS
TRANSPORTING
TREATMENT OF ALLOYS OR NON-FERROUS METALS
WORKING METALLIC POWDER
title POWDER FOR MAGNETIC CORE, POWDER-COMPACTED MAGNETIC CORE, AND THEIR PRODUCTION METHOD
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-03T13%3A01%3A37IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=CHOU%20KOKUHOU&rft.date=2005-06-09&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2005146315A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true