FLAMEPROOF FIBER, CARBON FIBER AND METHOD FOR PRODUCING THEM

PROBLEM TO BE SOLVED: To obtain a carbon fiber having excellent cost performance and a flameproof fiber suitable for obtaining the same and to provide methods for producing the flameproof fiber and the carbon fiber, which are suitable for producing them and have high productivity. SOLUTION: The meth...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ISE MASASHI, ENDO MAKOTO, HIGUCHI MICHINORI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ISE MASASHI
ENDO MAKOTO
HIGUCHI MICHINORI
description PROBLEM TO BE SOLVED: To obtain a carbon fiber having excellent cost performance and a flameproof fiber suitable for obtaining the same and to provide methods for producing the flameproof fiber and the carbon fiber, which are suitable for producing them and have high productivity. SOLUTION: The method for producing the flameproof fiber comprises heat-treating a precursor fiber in the presence of at least one kind of an organic compound at 50-400°C so that a weighting percentage represented by formula: weighting percentage=äWo×DR-Wp}/Wp×100 (Wo: flameproof fiber weight (g/m); Wp: precursor fiber weight (g/m); DR: total draw ratio in flameproof treatment) reaches 10-1,000%. COPYRIGHT: (C)2005,JPO&NCIPI
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2005113305A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2005113305A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2005113305A3</originalsourceid><addsrcrecordid>eNrjZLBx83H0dQ0I8vd3U3DzdHIN0lFwdgxy8veD8BQc_VwUfF1DPPxdFNz8gxSACl1CnT393BVCPFx9eRhY0xJzilN5oTQ3g5Kba4izh25qQX58anFBYnJqXmpJvFeAkYGBqaGhsbGBqaMxUYoAGqMpbw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>FLAMEPROOF FIBER, CARBON FIBER AND METHOD FOR PRODUCING THEM</title><source>esp@cenet</source><creator>ISE MASASHI ; ENDO MAKOTO ; HIGUCHI MICHINORI</creator><creatorcontrib>ISE MASASHI ; ENDO MAKOTO ; HIGUCHI MICHINORI</creatorcontrib><description>PROBLEM TO BE SOLVED: To obtain a carbon fiber having excellent cost performance and a flameproof fiber suitable for obtaining the same and to provide methods for producing the flameproof fiber and the carbon fiber, which are suitable for producing them and have high productivity. SOLUTION: The method for producing the flameproof fiber comprises heat-treating a precursor fiber in the presence of at least one kind of an organic compound at 50-400°C so that a weighting percentage represented by formula: weighting percentage=äWo×DR-Wp}/Wp×100 (Wo: flameproof fiber weight (g/m); Wp: precursor fiber weight (g/m); DR: total draw ratio in flameproof treatment) reaches 10-1,000%. COPYRIGHT: (C)2005,JPO&amp;NCIPI</description><edition>7</edition><language>eng</language><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS ; CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS ; NATURAL OR ARTIFICIAL THREADS OR FIBRES ; SPINNING ; TEXTILES</subject><creationdate>2005</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20050428&amp;DB=EPODOC&amp;CC=JP&amp;NR=2005113305A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25555,76308</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20050428&amp;DB=EPODOC&amp;CC=JP&amp;NR=2005113305A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ISE MASASHI</creatorcontrib><creatorcontrib>ENDO MAKOTO</creatorcontrib><creatorcontrib>HIGUCHI MICHINORI</creatorcontrib><title>FLAMEPROOF FIBER, CARBON FIBER AND METHOD FOR PRODUCING THEM</title><description>PROBLEM TO BE SOLVED: To obtain a carbon fiber having excellent cost performance and a flameproof fiber suitable for obtaining the same and to provide methods for producing the flameproof fiber and the carbon fiber, which are suitable for producing them and have high productivity. SOLUTION: The method for producing the flameproof fiber comprises heat-treating a precursor fiber in the presence of at least one kind of an organic compound at 50-400°C so that a weighting percentage represented by formula: weighting percentage=äWo×DR-Wp}/Wp×100 (Wo: flameproof fiber weight (g/m); Wp: precursor fiber weight (g/m); DR: total draw ratio in flameproof treatment) reaches 10-1,000%. COPYRIGHT: (C)2005,JPO&amp;NCIPI</description><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</subject><subject>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</subject><subject>NATURAL OR ARTIFICIAL THREADS OR FIBRES</subject><subject>SPINNING</subject><subject>TEXTILES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2005</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLBx83H0dQ0I8vd3U3DzdHIN0lFwdgxy8veD8BQc_VwUfF1DPPxdFNz8gxSACl1CnT393BVCPFx9eRhY0xJzilN5oTQ3g5Kba4izh25qQX58anFBYnJqXmpJvFeAkYGBqaGhsbGBqaMxUYoAGqMpbw</recordid><startdate>20050428</startdate><enddate>20050428</enddate><creator>ISE MASASHI</creator><creator>ENDO MAKOTO</creator><creator>HIGUCHI MICHINORI</creator><scope>EVB</scope></search><sort><creationdate>20050428</creationdate><title>FLAMEPROOF FIBER, CARBON FIBER AND METHOD FOR PRODUCING THEM</title><author>ISE MASASHI ; ENDO MAKOTO ; HIGUCHI MICHINORI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2005113305A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2005</creationdate><topic>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</topic><topic>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</topic><topic>NATURAL OR ARTIFICIAL THREADS OR FIBRES</topic><topic>SPINNING</topic><topic>TEXTILES</topic><toplevel>online_resources</toplevel><creatorcontrib>ISE MASASHI</creatorcontrib><creatorcontrib>ENDO MAKOTO</creatorcontrib><creatorcontrib>HIGUCHI MICHINORI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ISE MASASHI</au><au>ENDO MAKOTO</au><au>HIGUCHI MICHINORI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>FLAMEPROOF FIBER, CARBON FIBER AND METHOD FOR PRODUCING THEM</title><date>2005-04-28</date><risdate>2005</risdate><abstract>PROBLEM TO BE SOLVED: To obtain a carbon fiber having excellent cost performance and a flameproof fiber suitable for obtaining the same and to provide methods for producing the flameproof fiber and the carbon fiber, which are suitable for producing them and have high productivity. SOLUTION: The method for producing the flameproof fiber comprises heat-treating a precursor fiber in the presence of at least one kind of an organic compound at 50-400°C so that a weighting percentage represented by formula: weighting percentage=äWo×DR-Wp}/Wp×100 (Wo: flameproof fiber weight (g/m); Wp: precursor fiber weight (g/m); DR: total draw ratio in flameproof treatment) reaches 10-1,000%. COPYRIGHT: (C)2005,JPO&amp;NCIPI</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2005113305A
source esp@cenet
subjects APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS
CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS
NATURAL OR ARTIFICIAL THREADS OR FIBRES
SPINNING
TEXTILES
title FLAMEPROOF FIBER, CARBON FIBER AND METHOD FOR PRODUCING THEM
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-15T03%3A44%3A22IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ISE%20MASASHI&rft.date=2005-04-28&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2005113305A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true