METHOD FOR PRODUCING THICK AND THIN YARN

PROBLEM TO BE SOLVED: To provide a method for producing a polyester thick and thin yarn suitable for obtaining a cloth having a natural spot feeling and grain feeling and also an excellent soft, spun tone and bulged feeling on preparing the cloth, economically at a low cost and stably by using a dir...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TANAKA MATSUMI, MIYATA MASANOBU, TOMISAKA IKUO, KATSUMA KEITA, KATSUI JUICHI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a method for producing a polyester thick and thin yarn suitable for obtaining a cloth having a natural spot feeling and grain feeling and also an excellent soft, spun tone and bulged feeling on preparing the cloth, economically at a low cost and stably by using a direct spinning and stretching method. SOLUTION: This method for producing the thick and thin yarn is characterized by melt-ejecting a polyester containing ≥90 mol% ethylene terephthalate, then without imparting preliminary entwinement, imparting an oil agent while revolving the yarn, taking-in the yarn with a non-heated roller for controlling tension (PTR), then introducing into a heated first godet roller (GR1) by setting 1.02-1.05 peripheral speed ratio of the GR1 to PTR and performing stretching and heat-setting with the heat-setting second godet roller (GR2) so as to make 42-55% elongation at break. COPYRIGHT: (C)2005,JPO&NCIPI