FLEXIBLE POLYPROYLENE RESIN COMPOSITION
PROBLEM TO BE SOLVED: To provide a flexible polypropylene resin composition being lowly sticky and having excellent adhesiveness without detriment to flexibility and heat resistance. SOLUTION: The flexible polypropylene resin composition is prepared by melt-kneading (A) a propylene resin comprising...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | MORITA TATSUHIKO ENDO MASAHIKO KISHIDA TOYOJI |
description | PROBLEM TO BE SOLVED: To provide a flexible polypropylene resin composition being lowly sticky and having excellent adhesiveness without detriment to flexibility and heat resistance. SOLUTION: The flexible polypropylene resin composition is prepared by melt-kneading (A) a propylene resin comprising 10 to 95 mass% (a1) following propylene homopolymer (i) and/or copolymer containing at most 4 mol% other olefin units and 90 to 5 mass% (a2) propylene random copolymer having an [η] of 0.5 to 10 dL/g and containing 10 to 80 mol% units of an olefin other than propylene and (B) a polyolefin resin modified with, e.g., an unsaturated carboxylic acid. The above propylene homopolymer (i) satisfies (i) the [η] (at 135°C in decalin) is 0.5 to 10 dL/g, (ii) the boiling n-heptane-insolubles weight (W) is 10 to 99 mass%, and (iii) T2HR(80)≤670-2.2×W, and T2HR(80)/T2HR(30)≤8.8+0.086×W (wherein T2HR(30) and T2HR(80) are each the relaxation time (μs) of the rubber component as measured with pulsed NMR at 30°C or 80°C, and W is as defined above). COPYRIGHT: (C)2005,JPO&NCIPI |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2005097336A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2005097336A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2005097336A3</originalsourceid><addsrcrecordid>eNrjZFB383GN8HTycVUI8PeJDAjyj_Rx9XNVCHIN9vRTcPb3DfAP9gzx9PfjYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBgamBpbmxsZmjsZEKQIAW9ckug</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>FLEXIBLE POLYPROYLENE RESIN COMPOSITION</title><source>esp@cenet</source><creator>MORITA TATSUHIKO ; ENDO MASAHIKO ; KISHIDA TOYOJI</creator><creatorcontrib>MORITA TATSUHIKO ; ENDO MASAHIKO ; KISHIDA TOYOJI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a flexible polypropylene resin composition being lowly sticky and having excellent adhesiveness without detriment to flexibility and heat resistance. SOLUTION: The flexible polypropylene resin composition is prepared by melt-kneading (A) a propylene resin comprising 10 to 95 mass% (a1) following propylene homopolymer (i) and/or copolymer containing at most 4 mol% other olefin units and 90 to 5 mass% (a2) propylene random copolymer having an [η] of 0.5 to 10 dL/g and containing 10 to 80 mol% units of an olefin other than propylene and (B) a polyolefin resin modified with, e.g., an unsaturated carboxylic acid. The above propylene homopolymer (i) satisfies (i) the [η] (at 135°C in decalin) is 0.5 to 10 dL/g, (ii) the boiling n-heptane-insolubles weight (W) is 10 to 99 mass%, and (iii) T2HR(80)≤670-2.2×W, and T2HR(80)/T2HR(30)≤8.8+0.086×W (wherein T2HR(30) and T2HR(80) are each the relaxation time (μs) of the rubber component as measured with pulsed NMR at 30°C or 80°C, and W is as defined above). COPYRIGHT: (C)2005,JPO&NCIPI</description><edition>7</edition><language>eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2005</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20050414&DB=EPODOC&CC=JP&NR=2005097336A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20050414&DB=EPODOC&CC=JP&NR=2005097336A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MORITA TATSUHIKO</creatorcontrib><creatorcontrib>ENDO MASAHIKO</creatorcontrib><creatorcontrib>KISHIDA TOYOJI</creatorcontrib><title>FLEXIBLE POLYPROYLENE RESIN COMPOSITION</title><description>PROBLEM TO BE SOLVED: To provide a flexible polypropylene resin composition being lowly sticky and having excellent adhesiveness without detriment to flexibility and heat resistance. SOLUTION: The flexible polypropylene resin composition is prepared by melt-kneading (A) a propylene resin comprising 10 to 95 mass% (a1) following propylene homopolymer (i) and/or copolymer containing at most 4 mol% other olefin units and 90 to 5 mass% (a2) propylene random copolymer having an [η] of 0.5 to 10 dL/g and containing 10 to 80 mol% units of an olefin other than propylene and (B) a polyolefin resin modified with, e.g., an unsaturated carboxylic acid. The above propylene homopolymer (i) satisfies (i) the [η] (at 135°C in decalin) is 0.5 to 10 dL/g, (ii) the boiling n-heptane-insolubles weight (W) is 10 to 99 mass%, and (iii) T2HR(80)≤670-2.2×W, and T2HR(80)/T2HR(30)≤8.8+0.086×W (wherein T2HR(30) and T2HR(80) are each the relaxation time (μs) of the rubber component as measured with pulsed NMR at 30°C or 80°C, and W is as defined above). COPYRIGHT: (C)2005,JPO&NCIPI</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2005</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFB383GN8HTycVUI8PeJDAjyj_Rx9XNVCHIN9vRTcPb3DfAP9gzx9PfjYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBgamBpbmxsZmjsZEKQIAW9ckug</recordid><startdate>20050414</startdate><enddate>20050414</enddate><creator>MORITA TATSUHIKO</creator><creator>ENDO MASAHIKO</creator><creator>KISHIDA TOYOJI</creator><scope>EVB</scope></search><sort><creationdate>20050414</creationdate><title>FLEXIBLE POLYPROYLENE RESIN COMPOSITION</title><author>MORITA TATSUHIKO ; ENDO MASAHIKO ; KISHIDA TOYOJI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2005097336A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2005</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>MORITA TATSUHIKO</creatorcontrib><creatorcontrib>ENDO MASAHIKO</creatorcontrib><creatorcontrib>KISHIDA TOYOJI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MORITA TATSUHIKO</au><au>ENDO MASAHIKO</au><au>KISHIDA TOYOJI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>FLEXIBLE POLYPROYLENE RESIN COMPOSITION</title><date>2005-04-14</date><risdate>2005</risdate><abstract>PROBLEM TO BE SOLVED: To provide a flexible polypropylene resin composition being lowly sticky and having excellent adhesiveness without detriment to flexibility and heat resistance. SOLUTION: The flexible polypropylene resin composition is prepared by melt-kneading (A) a propylene resin comprising 10 to 95 mass% (a1) following propylene homopolymer (i) and/or copolymer containing at most 4 mol% other olefin units and 90 to 5 mass% (a2) propylene random copolymer having an [η] of 0.5 to 10 dL/g and containing 10 to 80 mol% units of an olefin other than propylene and (B) a polyolefin resin modified with, e.g., an unsaturated carboxylic acid. The above propylene homopolymer (i) satisfies (i) the [η] (at 135°C in decalin) is 0.5 to 10 dL/g, (ii) the boiling n-heptane-insolubles weight (W) is 10 to 99 mass%, and (iii) T2HR(80)≤670-2.2×W, and T2HR(80)/T2HR(30)≤8.8+0.086×W (wherein T2HR(30) and T2HR(80) are each the relaxation time (μs) of the rubber component as measured with pulsed NMR at 30°C or 80°C, and W is as defined above). COPYRIGHT: (C)2005,JPO&NCIPI</abstract><edition>7</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JP2005097336A |
source | esp@cenet |
subjects | CHEMISTRY COMPOSITIONS BASED THEREON COMPOSITIONS OF MACROMOLECULAR COMPOUNDS METALLURGY ORGANIC MACROMOLECULAR COMPOUNDS THEIR PREPARATION OR CHEMICAL WORKING-UP |
title | FLEXIBLE POLYPROYLENE RESIN COMPOSITION |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-12T06%3A34%3A18IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MORITA%20TATSUHIKO&rft.date=2005-04-14&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2005097336A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |