HIGH-STRENGTH Fe-Ni-Co ALLOY FOR SHADOW MASK
PROBLEM TO BE SOLVED: To enhance the drop impact strength of an Fe-Ni-Co alloy without adding an element for enhancing the strength. SOLUTION: The high-strength Fe-Ni-Co alloy for a shadow mask comprises, by mass%, 30-35% Ni, 2-8% Co, 0.50% or less Mn, and the balance being Fe and unavoidable impuri...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To enhance the drop impact strength of an Fe-Ni-Co alloy without adding an element for enhancing the strength. SOLUTION: The high-strength Fe-Ni-Co alloy for a shadow mask comprises, by mass%, 30-35% Ni, 2-8% Co, 0.50% or less Mn, and the balance being Fe and unavoidable impurities or accompanying elements (wherein the elements are 0.10% or less C, 0.10% or less Si, 0.05% or less Al, 0.005% or less S and 0.005% or less P); is formed of a rolling structure; when annealed at 750°C for 15 minutes, develops a recrystallized structure in which the grain size number is 9.5 or larger; and when annealed at 850°C for 15 minutes, develops a recrystallized structure in which the grain size number is 8.5 or larger. COPYRIGHT: (C)2005,JPO&NCIPI |
---|