SUPPRESSION METHOD FOR POWDERING OF SLAG
PROBLEM TO BE SOLVED: To provide a method for suppressing powdering of a slag and using the slag effectively. SOLUTION: The slag contains, as main components, silicon oxide, aluminum oxide and calcium oxide, and among the silicon oxide content x (%), the aluminum oxide content y (%), and the calcium...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide a method for suppressing powdering of a slag and using the slag effectively. SOLUTION: The slag contains, as main components, silicon oxide, aluminum oxide and calcium oxide, and among the silicon oxide content x (%), the aluminum oxide content y (%), and the calcium oxide content z (%), there are relations: formula (1) [z≥50, y>x, and x+y+z=100]. The suppression method for powdering the slag is cooling the slag to solidify from its melt state by a cooling speed V (°C/min) which satisfies the following relation on the contents of respective components: formula (2) [logV≥(10x-45)/(100-0.6x-y)]. COPYRIGHT: (C)2005,JPO&NCIPI |
---|