METHOD FOR MANUFACTURING PRIMARY COATED OPTICAL FIBER

PROBLEM TO BE SOLVED: To provide a method for manufacturing a primary coated optical fiber excellent in side pressure properties while controlling the variation of the coating diameter to ≤0.5 μm even in a high speed spinning at a linear velocity of >2,000 m/min. SOLUTION: A melt-spun primary opt...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: FUJIMAKI MUNEHISA, ONODERA MIGAKU
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator FUJIMAKI MUNEHISA
ONODERA MIGAKU
description PROBLEM TO BE SOLVED: To provide a method for manufacturing a primary coated optical fiber excellent in side pressure properties while controlling the variation of the coating diameter to ≤0.5 μm even in a high speed spinning at a linear velocity of >2,000 m/min. SOLUTION: A melt-spun primary optical fiber is coated with a resin to obtain the primary coated optical fiber. When the primary coated optical fiber is coiled via a turn pulley 21, the vibration of the turn pulley 21 is reduced to be ≤13 μm. Further, the eccentricity of the turn pulley 21 is reduced to be c×r2≤4×104äwhere c(μm) is the eccentricity and r(rpm) is the number of revolution}. COPYRIGHT: (C)2004,JPO&NCIPI
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2004203627A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2004203627A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2004203627A3</originalsourceid><addsrcrecordid>eNrjZDD1dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXCAjy9HUMilRw9ncMcXVR8A8I8XR29FFw83RyDeJhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGBiZGBsZmRuaOxkQpAgA7uSgI</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MANUFACTURING PRIMARY COATED OPTICAL FIBER</title><source>esp@cenet</source><creator>FUJIMAKI MUNEHISA ; ONODERA MIGAKU</creator><creatorcontrib>FUJIMAKI MUNEHISA ; ONODERA MIGAKU</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a method for manufacturing a primary coated optical fiber excellent in side pressure properties while controlling the variation of the coating diameter to ≤0.5 μm even in a high speed spinning at a linear velocity of &gt;2,000 m/min. SOLUTION: A melt-spun primary optical fiber is coated with a resin to obtain the primary coated optical fiber. When the primary coated optical fiber is coiled via a turn pulley 21, the vibration of the turn pulley 21 is reduced to be ≤13 μm. Further, the eccentricity of the turn pulley 21 is reduced to be c×r2≤4×104äwhere c(μm) is the eccentricity and r(rpm) is the number of revolution}. COPYRIGHT: (C)2004,JPO&amp;NCIPI</description><edition>7</edition><language>eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2004</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20040722&amp;DB=EPODOC&amp;CC=JP&amp;NR=2004203627A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20040722&amp;DB=EPODOC&amp;CC=JP&amp;NR=2004203627A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>FUJIMAKI MUNEHISA</creatorcontrib><creatorcontrib>ONODERA MIGAKU</creatorcontrib><title>METHOD FOR MANUFACTURING PRIMARY COATED OPTICAL FIBER</title><description>PROBLEM TO BE SOLVED: To provide a method for manufacturing a primary coated optical fiber excellent in side pressure properties while controlling the variation of the coating diameter to ≤0.5 μm even in a high speed spinning at a linear velocity of &gt;2,000 m/min. SOLUTION: A melt-spun primary optical fiber is coated with a resin to obtain the primary coated optical fiber. When the primary coated optical fiber is coiled via a turn pulley 21, the vibration of the turn pulley 21 is reduced to be ≤13 μm. Further, the eccentricity of the turn pulley 21 is reduced to be c×r2≤4×104äwhere c(μm) is the eccentricity and r(rpm) is the number of revolution}. COPYRIGHT: (C)2004,JPO&amp;NCIPI</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2004</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDD1dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXCAjy9HUMilRw9ncMcXVR8A8I8XR29FFw83RyDeJhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGBiZGBsZmRuaOxkQpAgA7uSgI</recordid><startdate>20040722</startdate><enddate>20040722</enddate><creator>FUJIMAKI MUNEHISA</creator><creator>ONODERA MIGAKU</creator><scope>EVB</scope></search><sort><creationdate>20040722</creationdate><title>METHOD FOR MANUFACTURING PRIMARY COATED OPTICAL FIBER</title><author>FUJIMAKI MUNEHISA ; ONODERA MIGAKU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2004203627A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2004</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>FUJIMAKI MUNEHISA</creatorcontrib><creatorcontrib>ONODERA MIGAKU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>FUJIMAKI MUNEHISA</au><au>ONODERA MIGAKU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MANUFACTURING PRIMARY COATED OPTICAL FIBER</title><date>2004-07-22</date><risdate>2004</risdate><abstract>PROBLEM TO BE SOLVED: To provide a method for manufacturing a primary coated optical fiber excellent in side pressure properties while controlling the variation of the coating diameter to ≤0.5 μm even in a high speed spinning at a linear velocity of &gt;2,000 m/min. SOLUTION: A melt-spun primary optical fiber is coated with a resin to obtain the primary coated optical fiber. When the primary coated optical fiber is coiled via a turn pulley 21, the vibration of the turn pulley 21 is reduced to be ≤13 μm. Further, the eccentricity of the turn pulley 21 is reduced to be c×r2≤4×104äwhere c(μm) is the eccentricity and r(rpm) is the number of revolution}. COPYRIGHT: (C)2004,JPO&amp;NCIPI</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2004203627A
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
METALLURGY
MINERAL OR SLAG WOOL
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title METHOD FOR MANUFACTURING PRIMARY COATED OPTICAL FIBER
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-05T13%3A33%3A41IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=FUJIMAKI%20MUNEHISA&rft.date=2004-07-22&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2004203627A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true