MANUFACTURING METHOD OF NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY

PROBLEM TO BE SOLVED: To provide a manufacturing method of non-aqueous electrolyte secondary battery having an improved charge/discharge cycle life. SOLUTION: The manufacturing method of a non-aqueous electrolyte secondary battery comprising a positive electrode, a negative electrode, non-aqueous so...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KAMIBAYASHI SHINICHI, SATO ASAKO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a manufacturing method of non-aqueous electrolyte secondary battery having an improved charge/discharge cycle life. SOLUTION: The manufacturing method of a non-aqueous electrolyte secondary battery comprising a positive electrode, a negative electrode, non-aqueous solvent, and a non-aqueous electrolyte containing a first electrolyte to be dissolved by the non-aqueous solvent, comprises a step of preparing slurry containing a positive electrode active material and a second electrolyte, and a step of coating the slurry to a collector. COPYRIGHT: (C)2004,JPO&NCIPI