CONTINUOUS CASTING METHOD OF STEEL

PROBLEM TO BE SOLVED: To cause no occurrence of inner crack in a cast piece, to uniformly disperse main segregation in a width direction and to reduce its occurrence. SOLUTION: Space of a support roll is gradually reduced so that the cast piece in whole width comes into contact with the roll until t...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KUMAKURA SEIJI, NOZAKI ISAO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To cause no occurrence of inner crack in a cast piece, to uniformly disperse main segregation in a width direction and to reduce its occurrence. SOLUTION: Space of a support roll is gradually reduced so that the cast piece in whole width comes into contact with the roll until thickness of a solidified shell becomes ≥70 mm. Then while bulging is applied till a position where a solidus line crater end appears, rolling reduction below bulging amount is applied. COPYRIGHT: (C)2004,JPO