METHOD FOR MANUFACTURING POWER FOR MAGNET
PROBLEM TO BE SOLVED: To solve the problem that, in most cases of conventional manufacturing methods of powder for a magnet, nitriding is applied to powder after grinding and resultantly oxygen molecules as well as nitrogen molecules are bonded to the powder and this bonding of oxygen causes deterio...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | TAKAI TSUTOMU KAMIYAMA MASAHIKO MIZOGUCHI TSUGIO HIRAGA KAZUHITO NAKAJIMA JUNJI |
description | PROBLEM TO BE SOLVED: To solve the problem that, in most cases of conventional manufacturing methods of powder for a magnet, nitriding is applied to powder after grinding and resultantly oxygen molecules as well as nitrogen molecules are bonded to the powder and this bonding of oxygen causes deterioration in the performance of a magnet. SOLUTION: Before coarse grinding of ST06, nitriding is carried out in ST05, that is, nitriding is performed in a stage of an ingot. Accordingly, the bonding of oxygen can be sufficiently suppressed, and magnetic properties can be maintained in an excellent state. COPYRIGHT: (C)2004,JPO |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2003321707A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2003321707A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2003321707A3</originalsourceid><addsrcrecordid>eNrjZND0dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXCPAPdw2Cirv7uYbwMLCmJeYUp_JCaW4GJTfXEGcP3dSC_PjU4oLE5NS81JJ4rwAjAwNjYyNDcwNzR2OiFAEAc2Qkwg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MANUFACTURING POWER FOR MAGNET</title><source>esp@cenet</source><creator>TAKAI TSUTOMU ; KAMIYAMA MASAHIKO ; MIZOGUCHI TSUGIO ; HIRAGA KAZUHITO ; NAKAJIMA JUNJI</creator><creatorcontrib>TAKAI TSUTOMU ; KAMIYAMA MASAHIKO ; MIZOGUCHI TSUGIO ; HIRAGA KAZUHITO ; NAKAJIMA JUNJI</creatorcontrib><description>PROBLEM TO BE SOLVED: To solve the problem that, in most cases of conventional manufacturing methods of powder for a magnet, nitriding is applied to powder after grinding and resultantly oxygen molecules as well as nitrogen molecules are bonded to the powder and this bonding of oxygen causes deterioration in the performance of a magnet. SOLUTION: Before coarse grinding of ST06, nitriding is carried out in ST05, that is, nitriding is performed in a stage of an ingot. Accordingly, the bonding of oxygen can be sufficiently suppressed, and magnetic properties can be maintained in an excellent state. COPYRIGHT: (C)2004,JPO</description><edition>7</edition><language>eng</language><subject>ALLOYS ; BASIC ELECTRIC ELEMENTS ; CASTING ; CHEMISTRY ; ELECTRICITY ; FERROUS OR NON-FERROUS ALLOYS ; INDUCTANCES ; MAGNETS ; MAKING METALLIC POWDER ; MANUFACTURE OF ARTICLES FROM METALLIC POWDER ; METALLURGY ; PERFORMING OPERATIONS ; POWDER METALLURGY ; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES ; TRANSFORMERS ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS ; WORKING METALLIC POWDER</subject><creationdate>2003</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20031114&DB=EPODOC&CC=JP&NR=2003321707A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20031114&DB=EPODOC&CC=JP&NR=2003321707A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TAKAI TSUTOMU</creatorcontrib><creatorcontrib>KAMIYAMA MASAHIKO</creatorcontrib><creatorcontrib>MIZOGUCHI TSUGIO</creatorcontrib><creatorcontrib>HIRAGA KAZUHITO</creatorcontrib><creatorcontrib>NAKAJIMA JUNJI</creatorcontrib><title>METHOD FOR MANUFACTURING POWER FOR MAGNET</title><description>PROBLEM TO BE SOLVED: To solve the problem that, in most cases of conventional manufacturing methods of powder for a magnet, nitriding is applied to powder after grinding and resultantly oxygen molecules as well as nitrogen molecules are bonded to the powder and this bonding of oxygen causes deterioration in the performance of a magnet. SOLUTION: Before coarse grinding of ST06, nitriding is carried out in ST05, that is, nitriding is performed in a stage of an ingot. Accordingly, the bonding of oxygen can be sufficiently suppressed, and magnetic properties can be maintained in an excellent state. COPYRIGHT: (C)2004,JPO</description><subject>ALLOYS</subject><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CASTING</subject><subject>CHEMISTRY</subject><subject>ELECTRICITY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>INDUCTANCES</subject><subject>MAGNETS</subject><subject>MAKING METALLIC POWDER</subject><subject>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES</subject><subject>TRANSFORMERS</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><subject>WORKING METALLIC POWDER</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2003</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZND0dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXCPAPdw2Cirv7uYbwMLCmJeYUp_JCaW4GJTfXEGcP3dSC_PjU4oLE5NS81JJ4rwAjAwNjYyNDcwNzR2OiFAEAc2Qkwg</recordid><startdate>20031114</startdate><enddate>20031114</enddate><creator>TAKAI TSUTOMU</creator><creator>KAMIYAMA MASAHIKO</creator><creator>MIZOGUCHI TSUGIO</creator><creator>HIRAGA KAZUHITO</creator><creator>NAKAJIMA JUNJI</creator><scope>EVB</scope></search><sort><creationdate>20031114</creationdate><title>METHOD FOR MANUFACTURING POWER FOR MAGNET</title><author>TAKAI TSUTOMU ; KAMIYAMA MASAHIKO ; MIZOGUCHI TSUGIO ; HIRAGA KAZUHITO ; NAKAJIMA JUNJI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2003321707A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2003</creationdate><topic>ALLOYS</topic><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CASTING</topic><topic>CHEMISTRY</topic><topic>ELECTRICITY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>INDUCTANCES</topic><topic>MAGNETS</topic><topic>MAKING METALLIC POWDER</topic><topic>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES</topic><topic>TRANSFORMERS</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><topic>WORKING METALLIC POWDER</topic><toplevel>online_resources</toplevel><creatorcontrib>TAKAI TSUTOMU</creatorcontrib><creatorcontrib>KAMIYAMA MASAHIKO</creatorcontrib><creatorcontrib>MIZOGUCHI TSUGIO</creatorcontrib><creatorcontrib>HIRAGA KAZUHITO</creatorcontrib><creatorcontrib>NAKAJIMA JUNJI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TAKAI TSUTOMU</au><au>KAMIYAMA MASAHIKO</au><au>MIZOGUCHI TSUGIO</au><au>HIRAGA KAZUHITO</au><au>NAKAJIMA JUNJI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MANUFACTURING POWER FOR MAGNET</title><date>2003-11-14</date><risdate>2003</risdate><abstract>PROBLEM TO BE SOLVED: To solve the problem that, in most cases of conventional manufacturing methods of powder for a magnet, nitriding is applied to powder after grinding and resultantly oxygen molecules as well as nitrogen molecules are bonded to the powder and this bonding of oxygen causes deterioration in the performance of a magnet. SOLUTION: Before coarse grinding of ST06, nitriding is carried out in ST05, that is, nitriding is performed in a stage of an ingot. Accordingly, the bonding of oxygen can be sufficiently suppressed, and magnetic properties can be maintained in an excellent state. COPYRIGHT: (C)2004,JPO</abstract><edition>7</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JP2003321707A |
source | esp@cenet |
subjects | ALLOYS BASIC ELECTRIC ELEMENTS CASTING CHEMISTRY ELECTRICITY FERROUS OR NON-FERROUS ALLOYS INDUCTANCES MAGNETS MAKING METALLIC POWDER MANUFACTURE OF ARTICLES FROM METALLIC POWDER METALLURGY PERFORMING OPERATIONS POWDER METALLURGY SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES TRANSFORMERS TRANSPORTING TREATMENT OF ALLOYS OR NON-FERROUS METALS WORKING METALLIC POWDER |
title | METHOD FOR MANUFACTURING POWER FOR MAGNET |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-19T23%3A30%3A00IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TAKAI%20TSUTOMU&rft.date=2003-11-14&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2003321707A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |