METHOD FOR MANUFACTURING CERAMICS MOLDED PRODUCT

PROBLEM TO BE SOLVED: To provide a method for manufacturing a ceramics molded product by which a defect and a deformation are prevented from being generated, when the product is baked. SOLUTION: A molding die 13 formed of a water-absorbing material is mounted on each of the mutually opposite faces o...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KATOU NOBUHISA, HIRAI TOSHIO, MIZUNO MASATOSHI, ITO MASATAKE, TAKAYAMA SADAJI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KATOU NOBUHISA
HIRAI TOSHIO
MIZUNO MASATOSHI
ITO MASATAKE
TAKAYAMA SADAJI
description PROBLEM TO BE SOLVED: To provide a method for manufacturing a ceramics molded product by which a defect and a deformation are prevented from being generated, when the product is baked. SOLUTION: A molding die 13 formed of a water-absorbing material is mounted on each of the mutually opposite faces of a pair of mold clamping plates 12, and a molding recessed part 14 is formed on each of the mutually opposite faces of the paired molding dies 13. On one of the mold clamping plates 12, a rotary supporting shaft 16 whose rotary axis 15 extends in the horizontal direction is fitted to the center of an opposite face to the face on which the molding die 13 is mounted. In the molding die 13 mounted on the other mold clamping plate 12, a first insertion hole 17 through which an injection pipe 18 with an injection hole is inserted, is formed through. Further, a ceramics slurry is injected into the molding recessed part 14 from the injection hole in such a state that the paired molding dies 13 rotate pivoted on the rotary axis 15, and thus the ceramics molded product is molded. Finally, the paired molding dies 13 are opened apart to release said product. COPYRIGHT: (C)2004,JPO
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2003291120A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2003291120A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2003291120A3</originalsourceid><addsrcrecordid>eNrjZDDwdQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXcHYNcvT1dA5W8PX3cXF1UQgI8ncJdQ7hYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBgbGRpaGhkYGjsZEKQIAerAmrA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MANUFACTURING CERAMICS MOLDED PRODUCT</title><source>esp@cenet</source><creator>KATOU NOBUHISA ; HIRAI TOSHIO ; MIZUNO MASATOSHI ; ITO MASATAKE ; TAKAYAMA SADAJI</creator><creatorcontrib>KATOU NOBUHISA ; HIRAI TOSHIO ; MIZUNO MASATOSHI ; ITO MASATAKE ; TAKAYAMA SADAJI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a method for manufacturing a ceramics molded product by which a defect and a deformation are prevented from being generated, when the product is baked. SOLUTION: A molding die 13 formed of a water-absorbing material is mounted on each of the mutually opposite faces of a pair of mold clamping plates 12, and a molding recessed part 14 is formed on each of the mutually opposite faces of the paired molding dies 13. On one of the mold clamping plates 12, a rotary supporting shaft 16 whose rotary axis 15 extends in the horizontal direction is fitted to the center of an opposite face to the face on which the molding die 13 is mounted. In the molding die 13 mounted on the other mold clamping plate 12, a first insertion hole 17 through which an injection pipe 18 with an injection hole is inserted, is formed through. Further, a ceramics slurry is injected into the molding recessed part 14 from the injection hole in such a state that the paired molding dies 13 rotate pivoted on the rotary axis 15, and thus the ceramics molded product is molded. Finally, the paired molding dies 13 are opened apart to release said product. COPYRIGHT: (C)2004,JPO</description><edition>7</edition><language>eng</language><subject>PERFORMING OPERATIONS ; SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER ; TRANSPORTING ; WORKING CEMENT, CLAY, OR STONE</subject><creationdate>2003</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20031014&amp;DB=EPODOC&amp;CC=JP&amp;NR=2003291120A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20031014&amp;DB=EPODOC&amp;CC=JP&amp;NR=2003291120A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KATOU NOBUHISA</creatorcontrib><creatorcontrib>HIRAI TOSHIO</creatorcontrib><creatorcontrib>MIZUNO MASATOSHI</creatorcontrib><creatorcontrib>ITO MASATAKE</creatorcontrib><creatorcontrib>TAKAYAMA SADAJI</creatorcontrib><title>METHOD FOR MANUFACTURING CERAMICS MOLDED PRODUCT</title><description>PROBLEM TO BE SOLVED: To provide a method for manufacturing a ceramics molded product by which a defect and a deformation are prevented from being generated, when the product is baked. SOLUTION: A molding die 13 formed of a water-absorbing material is mounted on each of the mutually opposite faces of a pair of mold clamping plates 12, and a molding recessed part 14 is formed on each of the mutually opposite faces of the paired molding dies 13. On one of the mold clamping plates 12, a rotary supporting shaft 16 whose rotary axis 15 extends in the horizontal direction is fitted to the center of an opposite face to the face on which the molding die 13 is mounted. In the molding die 13 mounted on the other mold clamping plate 12, a first insertion hole 17 through which an injection pipe 18 with an injection hole is inserted, is formed through. Further, a ceramics slurry is injected into the molding recessed part 14 from the injection hole in such a state that the paired molding dies 13 rotate pivoted on the rotary axis 15, and thus the ceramics molded product is molded. Finally, the paired molding dies 13 are opened apart to release said product. COPYRIGHT: (C)2004,JPO</description><subject>PERFORMING OPERATIONS</subject><subject>SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER</subject><subject>TRANSPORTING</subject><subject>WORKING CEMENT, CLAY, OR STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2003</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDDwdQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXcHYNcvT1dA5W8PX3cXF1UQgI8ncJdQ7hYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBgbGRpaGhkYGjsZEKQIAerAmrA</recordid><startdate>20031014</startdate><enddate>20031014</enddate><creator>KATOU NOBUHISA</creator><creator>HIRAI TOSHIO</creator><creator>MIZUNO MASATOSHI</creator><creator>ITO MASATAKE</creator><creator>TAKAYAMA SADAJI</creator><scope>EVB</scope></search><sort><creationdate>20031014</creationdate><title>METHOD FOR MANUFACTURING CERAMICS MOLDED PRODUCT</title><author>KATOU NOBUHISA ; HIRAI TOSHIO ; MIZUNO MASATOSHI ; ITO MASATAKE ; TAKAYAMA SADAJI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2003291120A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2003</creationdate><topic>PERFORMING OPERATIONS</topic><topic>SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER</topic><topic>TRANSPORTING</topic><topic>WORKING CEMENT, CLAY, OR STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>KATOU NOBUHISA</creatorcontrib><creatorcontrib>HIRAI TOSHIO</creatorcontrib><creatorcontrib>MIZUNO MASATOSHI</creatorcontrib><creatorcontrib>ITO MASATAKE</creatorcontrib><creatorcontrib>TAKAYAMA SADAJI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KATOU NOBUHISA</au><au>HIRAI TOSHIO</au><au>MIZUNO MASATOSHI</au><au>ITO MASATAKE</au><au>TAKAYAMA SADAJI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MANUFACTURING CERAMICS MOLDED PRODUCT</title><date>2003-10-14</date><risdate>2003</risdate><abstract>PROBLEM TO BE SOLVED: To provide a method for manufacturing a ceramics molded product by which a defect and a deformation are prevented from being generated, when the product is baked. SOLUTION: A molding die 13 formed of a water-absorbing material is mounted on each of the mutually opposite faces of a pair of mold clamping plates 12, and a molding recessed part 14 is formed on each of the mutually opposite faces of the paired molding dies 13. On one of the mold clamping plates 12, a rotary supporting shaft 16 whose rotary axis 15 extends in the horizontal direction is fitted to the center of an opposite face to the face on which the molding die 13 is mounted. In the molding die 13 mounted on the other mold clamping plate 12, a first insertion hole 17 through which an injection pipe 18 with an injection hole is inserted, is formed through. Further, a ceramics slurry is injected into the molding recessed part 14 from the injection hole in such a state that the paired molding dies 13 rotate pivoted on the rotary axis 15, and thus the ceramics molded product is molded. Finally, the paired molding dies 13 are opened apart to release said product. COPYRIGHT: (C)2004,JPO</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2003291120A
source esp@cenet
subjects PERFORMING OPERATIONS
SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER
TRANSPORTING
WORKING CEMENT, CLAY, OR STONE
title METHOD FOR MANUFACTURING CERAMICS MOLDED PRODUCT
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-01T09%3A13%3A49IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KATOU%20NOBUHISA&rft.date=2003-10-14&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2003291120A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true