COMPACT FOR CLEANING AND PRODUCTION METHOD THEREFOR
PROBLEM TO BE SOLVED: To provide a compact for cleaning which can be compacted into a desired shape without forcing out the adsorption and reduction functions of charcoal, and to provide a production method therefor. SOLUTION: By weight, 5 to 95% charcoal powder carbonized at a carbonization tempera...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide a compact for cleaning which can be compacted into a desired shape without forcing out the adsorption and reduction functions of charcoal, and to provide a production method therefor. SOLUTION: By weight, 5 to 95% charcoal powder carbonized at a carbonization temperature of 400 to 2,200°C, and 95 to 5% powder of diatomaceous shale are stirred and mixed to prepare a mixed composition as an aggregate of granular bodies of ≤1,000 μm. This mixed composition is filled into a compacting die, and is solidified. The solidified compact is fired at ≥600°C in a reducing atmosphere to obtain a compact for cleaning. Instead of diatomaceous shale, kaolinite and peat can be used. It is preferable that the prepared mixed composition is charged to the inside of water to be made into a slurried suspension, and is scooped up with a sheet making die, and is dried and solidified so as to be made into a compact. In particular, NOX and NO2as harmful substances in a vapor phase are converted into harmless N2. COPYRIGHT: (C)2003,JPO |
---|