METHOD OF MANUFACTURING OPTICAL GLASS AND COLORED GLASS AT LOW TEMPERATURE

PROBLEM TO BE SOLVED: To provide a manufacturing method for optical glass using an MX doped substance, which is friendly to the environment, high in effect to cost, and high in energy efficiency. SOLUTION: The method of manufacturing the optical glass and colored glass from a base material containin...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KOLBERG UWE, GIERKE MONIKA, CLASEN ROLF, FREUND JOCHEN, HENTSCHEL RUEDIGER
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KOLBERG UWE
GIERKE MONIKA
CLASEN ROLF
FREUND JOCHEN
HENTSCHEL RUEDIGER
description PROBLEM TO BE SOLVED: To provide a manufacturing method for optical glass using an MX doped substance, which is friendly to the environment, high in effect to cost, and high in energy efficiency. SOLUTION: The method of manufacturing the optical glass and colored glass from a base material containing at least SiO2powder or, together with an additive for lowering temperature for fluid phase sintering process than that of quartz glass or an additive for changing quartz glass performance using fluid phase sintering is characterized in the following steps: a step for making a suspension in which the starting materials are dissolved in an arbitary order as much as possible, and the insoluble materials are dispersed as much as possible; a step for manufacturing a green matter from the starting materials dissolved and dispersed; a step for drying the green matter; a step for liquid phase sintering the dried green matter at ≤1,200°C, preferably in a temperature range of 600-1,200°C. COPYRIGHT: (C)2003,JPO
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2003160374A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2003160374A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2003160374A3</originalsourceid><addsrcrecordid>eNrjZPDydQ3x8HdR8HdT8HX0C3VzdA4JDfL0c1fwDwjxdHb0UXD3cQwOVnD0c1Fw9vfxD3J1gYmEKPj4hyuEuPoGuAY5AjW58jCwpiXmFKfyQmluBiU31xBnD93Ugvz41OKCxOTUvNSSeK8AIwMDY0MzA2NzE0djohQBAKmMLbM</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF MANUFACTURING OPTICAL GLASS AND COLORED GLASS AT LOW TEMPERATURE</title><source>esp@cenet</source><creator>KOLBERG UWE ; GIERKE MONIKA ; CLASEN ROLF ; FREUND JOCHEN ; HENTSCHEL RUEDIGER</creator><creatorcontrib>KOLBERG UWE ; GIERKE MONIKA ; CLASEN ROLF ; FREUND JOCHEN ; HENTSCHEL RUEDIGER</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a manufacturing method for optical glass using an MX doped substance, which is friendly to the environment, high in effect to cost, and high in energy efficiency. SOLUTION: The method of manufacturing the optical glass and colored glass from a base material containing at least SiO2powder or, together with an additive for lowering temperature for fluid phase sintering process than that of quartz glass or an additive for changing quartz glass performance using fluid phase sintering is characterized in the following steps: a step for making a suspension in which the starting materials are dissolved in an arbitary order as much as possible, and the insoluble materials are dispersed as much as possible; a step for manufacturing a green matter from the starting materials dissolved and dispersed; a step for drying the green matter; a step for liquid phase sintering the dried green matter at ≤1,200°C, preferably in a temperature range of 600-1,200°C. COPYRIGHT: (C)2003,JPO</description><edition>7</edition><language>eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; LIME, MAGNESIA ; MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES ; METALLURGY ; MINERAL OR SLAG WOOL ; OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS ; OPTICS ; PHYSICS ; REFRACTORIES ; SLAG ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS ; TREATMENT OF NATURAL STONE</subject><creationdate>2003</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20030603&amp;DB=EPODOC&amp;CC=JP&amp;NR=2003160374A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20030603&amp;DB=EPODOC&amp;CC=JP&amp;NR=2003160374A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KOLBERG UWE</creatorcontrib><creatorcontrib>GIERKE MONIKA</creatorcontrib><creatorcontrib>CLASEN ROLF</creatorcontrib><creatorcontrib>FREUND JOCHEN</creatorcontrib><creatorcontrib>HENTSCHEL RUEDIGER</creatorcontrib><title>METHOD OF MANUFACTURING OPTICAL GLASS AND COLORED GLASS AT LOW TEMPERATURE</title><description>PROBLEM TO BE SOLVED: To provide a manufacturing method for optical glass using an MX doped substance, which is friendly to the environment, high in effect to cost, and high in energy efficiency. SOLUTION: The method of manufacturing the optical glass and colored glass from a base material containing at least SiO2powder or, together with an additive for lowering temperature for fluid phase sintering process than that of quartz glass or an additive for changing quartz glass performance using fluid phase sintering is characterized in the following steps: a step for making a suspension in which the starting materials are dissolved in an arbitary order as much as possible, and the insoluble materials are dispersed as much as possible; a step for manufacturing a green matter from the starting materials dissolved and dispersed; a step for drying the green matter; a step for liquid phase sintering the dried green matter at ≤1,200°C, preferably in a temperature range of 600-1,200°C. COPYRIGHT: (C)2003,JPO</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>LIME, MAGNESIA</subject><subject>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</subject><subject>OPTICS</subject><subject>PHYSICS</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2003</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPDydQ3x8HdR8HdT8HX0C3VzdA4JDfL0c1fwDwjxdHb0UXD3cQwOVnD0c1Fw9vfxD3J1gYmEKPj4hyuEuPoGuAY5AjW58jCwpiXmFKfyQmluBiU31xBnD93Ugvz41OKCxOTUvNSSeK8AIwMDY0MzA2NzE0djohQBAKmMLbM</recordid><startdate>20030603</startdate><enddate>20030603</enddate><creator>KOLBERG UWE</creator><creator>GIERKE MONIKA</creator><creator>CLASEN ROLF</creator><creator>FREUND JOCHEN</creator><creator>HENTSCHEL RUEDIGER</creator><scope>EVB</scope></search><sort><creationdate>20030603</creationdate><title>METHOD OF MANUFACTURING OPTICAL GLASS AND COLORED GLASS AT LOW TEMPERATURE</title><author>KOLBERG UWE ; GIERKE MONIKA ; CLASEN ROLF ; FREUND JOCHEN ; HENTSCHEL RUEDIGER</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2003160374A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2003</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>LIME, MAGNESIA</topic><topic>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</topic><topic>OPTICS</topic><topic>PHYSICS</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>KOLBERG UWE</creatorcontrib><creatorcontrib>GIERKE MONIKA</creatorcontrib><creatorcontrib>CLASEN ROLF</creatorcontrib><creatorcontrib>FREUND JOCHEN</creatorcontrib><creatorcontrib>HENTSCHEL RUEDIGER</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KOLBERG UWE</au><au>GIERKE MONIKA</au><au>CLASEN ROLF</au><au>FREUND JOCHEN</au><au>HENTSCHEL RUEDIGER</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF MANUFACTURING OPTICAL GLASS AND COLORED GLASS AT LOW TEMPERATURE</title><date>2003-06-03</date><risdate>2003</risdate><abstract>PROBLEM TO BE SOLVED: To provide a manufacturing method for optical glass using an MX doped substance, which is friendly to the environment, high in effect to cost, and high in energy efficiency. SOLUTION: The method of manufacturing the optical glass and colored glass from a base material containing at least SiO2powder or, together with an additive for lowering temperature for fluid phase sintering process than that of quartz glass or an additive for changing quartz glass performance using fluid phase sintering is characterized in the following steps: a step for making a suspension in which the starting materials are dissolved in an arbitary order as much as possible, and the insoluble materials are dispersed as much as possible; a step for manufacturing a green matter from the starting materials dissolved and dispersed; a step for drying the green matter; a step for liquid phase sintering the dried green matter at ≤1,200°C, preferably in a temperature range of 600-1,200°C. COPYRIGHT: (C)2003,JPO</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2003160374A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
LIME, MAGNESIA
MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
METALLURGY
MINERAL OR SLAG WOOL
OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS
OPTICS
PHYSICS
REFRACTORIES
SLAG
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
TREATMENT OF NATURAL STONE
title METHOD OF MANUFACTURING OPTICAL GLASS AND COLORED GLASS AT LOW TEMPERATURE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T23%3A57%3A26IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KOLBERG%20UWE&rft.date=2003-06-03&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2003160374A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true