METHOD FOR OBTAINING SINTERED METAL POWDER COMPACT

PROBLEM TO BE SOLVED: To prevent alumina contamination in method for obtaining sintered compacts of metal powder by the use of an alumina tray, and to manufacture the sintered compacts having excellent external surface appearance. SOLUTION: In this method for sintering metal-powder green bodies, an...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: NAKAI MASUMI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To prevent alumina contamination in method for obtaining sintered compacts of metal powder by the use of an alumina tray, and to manufacture the sintered compacts having excellent external surface appearance. SOLUTION: In this method for sintering metal-powder green bodies, an aqueous solution or alcoholic solution of magnesium nitrate hexahydrate is applied to the aluminum tray for placing the green bodies thereon and then sintering is carried out. Further, the powder-metal green bodies are metal injection molded green bodies.