METHOD FOR PRODUCING CRYSTALLINE BARIUM TITANATE POWDER

PROBLEM TO BE SOLVED: To provide a method for producing spherical ultrafine powder of crystalline barium titanate having a small particle diameter. SOLUTION: A sol precursor prepared using a partial acyloxy-titanium alkoxide and a barium compound is spayed on a strong alkali solution to cause coprec...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: U KOSHI, KIN EIDAI, CHIN SOSHUN, LEE SANG-KYUN, SAI KOSHIN, CHO EISHO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator U KOSHI
KIN EIDAI
CHIN SOSHUN
LEE SANG-KYUN
SAI KOSHIN
CHO EISHO
description PROBLEM TO BE SOLVED: To provide a method for producing spherical ultrafine powder of crystalline barium titanate having a small particle diameter. SOLUTION: A sol precursor prepared using a partial acyloxy-titanium alkoxide and a barium compound is spayed on a strong alkali solution to cause coprecipitation and barium titanate powder is crystallized from the resulting precipitate-containing solution and refined in a washing step to produce the objective crystalline barium titanate powder.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2002029745A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2002029745A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2002029745A3</originalsourceid><addsrcrecordid>eNrjZDD3dQ3x8HdRcPMPUggI8ncJdfb0c1dwDooMDnH08fH0c1VwcgzyDPVVCPEMcfRzDHFVCPAPd3EN4mFgTUvMKU7lhdLcDEpuriHOHrqpBfnxqcUFicmpeakl8V4BRgYGRgZGluYmpo7GRCkCAKMiKNg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PRODUCING CRYSTALLINE BARIUM TITANATE POWDER</title><source>esp@cenet</source><creator>U KOSHI ; KIN EIDAI ; CHIN SOSHUN ; LEE SANG-KYUN ; SAI KOSHIN ; CHO EISHO</creator><creatorcontrib>U KOSHI ; KIN EIDAI ; CHIN SOSHUN ; LEE SANG-KYUN ; SAI KOSHIN ; CHO EISHO</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a method for producing spherical ultrafine powder of crystalline barium titanate having a small particle diameter. SOLUTION: A sol precursor prepared using a partial acyloxy-titanium alkoxide and a barium compound is spayed on a strong alkali solution to cause coprecipitation and barium titanate powder is crystallized from the resulting precipitate-containing solution and refined in a washing step to produce the objective crystalline barium titanate powder.</description><edition>7</edition><language>eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; CONCRETE ; INORGANIC CHEMISTRY ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2002</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20020129&amp;DB=EPODOC&amp;CC=JP&amp;NR=2002029745A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20020129&amp;DB=EPODOC&amp;CC=JP&amp;NR=2002029745A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>U KOSHI</creatorcontrib><creatorcontrib>KIN EIDAI</creatorcontrib><creatorcontrib>CHIN SOSHUN</creatorcontrib><creatorcontrib>LEE SANG-KYUN</creatorcontrib><creatorcontrib>SAI KOSHIN</creatorcontrib><creatorcontrib>CHO EISHO</creatorcontrib><title>METHOD FOR PRODUCING CRYSTALLINE BARIUM TITANATE POWDER</title><description>PROBLEM TO BE SOLVED: To provide a method for producing spherical ultrafine powder of crystalline barium titanate having a small particle diameter. SOLUTION: A sol precursor prepared using a partial acyloxy-titanium alkoxide and a barium compound is spayed on a strong alkali solution to cause coprecipitation and barium titanate powder is crystallized from the resulting precipitate-containing solution and refined in a washing step to produce the objective crystalline barium titanate powder.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>CONCRETE</subject><subject>INORGANIC CHEMISTRY</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2002</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDD3dQ3x8HdRcPMPUggI8ncJdfb0c1dwDooMDnH08fH0c1VwcgzyDPVVCPEMcfRzDHFVCPAPd3EN4mFgTUvMKU7lhdLcDEpuriHOHrqpBfnxqcUFicmpeakl8V4BRgYGRgZGluYmpo7GRCkCAKMiKNg</recordid><startdate>20020129</startdate><enddate>20020129</enddate><creator>U KOSHI</creator><creator>KIN EIDAI</creator><creator>CHIN SOSHUN</creator><creator>LEE SANG-KYUN</creator><creator>SAI KOSHIN</creator><creator>CHO EISHO</creator><scope>EVB</scope></search><sort><creationdate>20020129</creationdate><title>METHOD FOR PRODUCING CRYSTALLINE BARIUM TITANATE POWDER</title><author>U KOSHI ; KIN EIDAI ; CHIN SOSHUN ; LEE SANG-KYUN ; SAI KOSHIN ; CHO EISHO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2002029745A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2002</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>CONCRETE</topic><topic>INORGANIC CHEMISTRY</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>U KOSHI</creatorcontrib><creatorcontrib>KIN EIDAI</creatorcontrib><creatorcontrib>CHIN SOSHUN</creatorcontrib><creatorcontrib>LEE SANG-KYUN</creatorcontrib><creatorcontrib>SAI KOSHIN</creatorcontrib><creatorcontrib>CHO EISHO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>U KOSHI</au><au>KIN EIDAI</au><au>CHIN SOSHUN</au><au>LEE SANG-KYUN</au><au>SAI KOSHIN</au><au>CHO EISHO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PRODUCING CRYSTALLINE BARIUM TITANATE POWDER</title><date>2002-01-29</date><risdate>2002</risdate><abstract>PROBLEM TO BE SOLVED: To provide a method for producing spherical ultrafine powder of crystalline barium titanate having a small particle diameter. SOLUTION: A sol precursor prepared using a partial acyloxy-titanium alkoxide and a barium compound is spayed on a strong alkali solution to cause coprecipitation and barium titanate powder is crystallized from the resulting precipitate-containing solution and refined in a washing step to produce the objective crystalline barium titanate powder.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2002029745A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
CONCRETE
INORGANIC CHEMISTRY
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title METHOD FOR PRODUCING CRYSTALLINE BARIUM TITANATE POWDER
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-05T23%3A30%3A22IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=U%20KOSHI&rft.date=2002-01-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2002029745A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true