HARDENABLE MARTENSITIC HEAT TREATED STEEL AND METHOD FOR HEAT TREATING THE STEEL

PROBLEM TO BE SOLVED: To obtain hardenable martensitic heat treated steel exhibiting increased heat resistance at 300 to 600 deg.C compared with the case of steel X12 CrNiMo12 and having high ductility. SOLUTION: This steel has the following composition of, by mass, 9 to 13% Cr, 0.001 to 0.25% Mn, 2...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GOECMEN ALKAN, ERNST PETER DR
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To obtain hardenable martensitic heat treated steel exhibiting increased heat resistance at 300 to 600 deg.C compared with the case of steel X12 CrNiMo12 and having high ductility. SOLUTION: This steel has the following composition of, by mass, 9 to 13% Cr, 0.001 to 0.25% Mn, 2 to 7% Ni, 0.001 to 8% Co, at least one of W and Mo by 0.5 to 4% in total, 0.5 to 0.8% V, at least one selected from Nb, Ta, Zr and Hf by 0.001 to 0.1% in total, 0.001 to 0.05% Ti, 0.001 to 0.15% Si, 0.01 to 0.1% C, 0.12 to 0.18% N,