METHOD FOR MANUFACTURING WATER GRANULATED SLAG

PROBLEM TO BE SOLVED: To obtain a high crushing characteristic by blowing steam against molten slag before being cooled by cooling water. SOLUTION: Molten slag 10 discharged from the main body 1 of a blast furnace is cooled by cooling water from a water injection nozzle 4a to manufacture water granu...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YANAGAWA TOSHIO, OKU NORIAKI, CHIBA HIROYUKI, MATSUYAMA KAZUHIKO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To obtain a high crushing characteristic by blowing steam against molten slag before being cooled by cooling water. SOLUTION: Molten slag 10 discharged from the main body 1 of a blast furnace is cooled by cooling water from a water injection nozzle 4a to manufacture water granulated slag. In the process, steam 20 is blown against the molten slag 10 before being cooled by the cooling water.