SLIMICIDE
PROBLEM TO BE SOLVED: To obtain a slimicide capable of releasing an antibacterial agent in a uniformly controlled elution condition for a long period of time, capable of dispelling inconvenience about measurement and excellent in transportation and handling. SOLUTION: This slimicide is produced by t...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To obtain a slimicide capable of releasing an antibacterial agent in a uniformly controlled elution condition for a long period of time, capable of dispelling inconvenience about measurement and excellent in transportation and handling. SOLUTION: This slimicide is produced by the pressure forming of an inclusion compound comprising an antibacterial agent and a multimolecular host compound together with at least one base material selected from the group consisting of phosphoric acid hydrogen calcium dihydrate, phosphoric acid tricalcium anhydride, phosphoric acid hydrogen magnesium trihydrate, phosphoric acid hydrogen magnesium octahydrate, vanillin, calcium citrate tetrahydrate, calcium sulfate dihydrate, calcium sulfate hemihydrate, acetoacetanilide, acetoacetic acid-o-toluidide, acetoacetic acid-p-toluidide, acetoacetic acid-o- anisidide, glyceryl monofatty acid ester, an alkyl sorbitan ester (having the HLB of |
---|