MELAMINE RESIN FOAM

PROBLEM TO BE SOLVED: To obtain an open-cell foam exhibiting decreased oil and water absorption by coating the whole or a part of the surface of a resin having a cellular structure with a fluoroalkyl ester. SOLUTION: Preferably, an amount of a fluoroalkyl ester applied is 0.001-5 mass %, and the flu...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: STOEHR DIETER, LENZ WERNER DR
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To obtain an open-cell foam exhibiting decreased oil and water absorption by coating the whole or a part of the surface of a resin having a cellular structure with a fluoroalkyl ester. SOLUTION: Preferably, an amount of a fluoroalkyl ester applied is 0.001-5 mass %, and the fluoroalkyl ester is preferably a completely fluorinated one. Preferably, the fluoroalkyl ester is a completely fluorinated 1-10C alkyl ester of acrylic acid, methacrylic acid, polyacrylic acid, polymethacrylic acid, phosphoric acid, or a 1-6C fatty acid. The objective foam is prepared by immersing a melamine resin foam in a milky aqueous solution of a fluoroalkyl ester or spraying the solution into the foam, then squeezing the foam to remove an excess of the solution, and drying the foam at 40-200 deg.C. The concentration of the milky solution used is preferably 0.1-20 mass %.