TRANSPARENT BIAXIALLY ORIENTED FILM

PROBLEM TO BE SOLVED: To obtain a biaxially oriented film excellent in orientation, mechanical and optical properties and having especially high UV stability, having a thermoplastic resin as the basic constituent, and useful as a partition film for illumination or the like, by making its thickness r...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: OBERLAENDER KLAUS, MURSCHALL URSULA, CRASS GUENTHER, BEWER GUENTER
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To obtain a biaxially oriented film excellent in orientation, mechanical and optical properties and having especially high UV stability, having a thermoplastic resin as the basic constituent, and useful as a partition film for illumination or the like, by making its thickness range specific and the film include UV stabilizer and gloss agent. SOLUTION: This film, with a thickness of 1-500 μm, is obtained by including (A) a crystalline thermoplastic resin such as preferably polyethylene terephthalate as the basic constituent, (B) at least one kind of a UV stabilizer [preferably 2-(4,6-diphenyl-1,3,5-triazin-2-yl)-5-(hexyl)oxyphenol or the like] and (C) at least one kind of a gloss agent (preferably bisbenzoxazole or the like). This film is obtained by melting the component A together with the component B and C in an extruder, extruding the resultant blend onto a cooling roller, biaxially orienting the blend thus extruded, heat-setting thus oriented film, and then winding the film. The component B to be included is preferably at 0.01-5 wt.% based on the component A.