PRODUCTION OF LITHIUM PHOSPHOTITANATE SINTERED BODY

PROBLEM TO BE SOLVED: To obtain a high lithium ion conductive inorganic solid electrolyte in a short-time single stage at a low temperature by supplying a DC pulsating current to a powdery mixture of an Li feed source, a Ti feed source and a P feed source under pressure. SOLUTION: As a Li feed sourc...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TABUCHI MITSUHARU, TAKEUCHI TOMONARI, ATO KAZUAKI, KAGEYAMA HIROYUKI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator TABUCHI MITSUHARU
TAKEUCHI TOMONARI
ATO KAZUAKI
KAGEYAMA HIROYUKI
description PROBLEM TO BE SOLVED: To obtain a high lithium ion conductive inorganic solid electrolyte in a short-time single stage at a low temperature by supplying a DC pulsating current to a powdery mixture of an Li feed source, a Ti feed source and a P feed source under pressure. SOLUTION: As a Li feed source is exemplified, e.g. LiOH, LiOH.H2O, Li2CO3 or LiNO3. As a Ti feed source is exemplified, e.g. H2TiO3, TiO2 or Ti(SO4)2. As a P feed source is, e.g. H3PO4, Li3PO4 or H3PO2. The molar ratio among the Li, Ti and P feed sources is preferably about (5-20):(10-30):(25-45). A powdery starting material mixture is prepared by mixing and agitating the powdery Li, Ti and P feed sources in an aqueous medium. An about 200-500A DC pulsating current is supplied to the mixture under about 5-40 MPa pressure and the mixture is brought into solid phase reaction at about 250-1,000 deg.C for about 2-10 min.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2000109360A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2000109360A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2000109360A3</originalsourceid><addsrcrecordid>eNrjZDAOCPJ3CXUO8fT3U_B3U_DxDPHwDPVVCPDwDwbiEM8QRz_HEFeFYE-_ENcgVxcFJ3-XSB4G1rTEnOJUXijNzaDk5hri7KGbWpAfn1pckJicmpdaEu8VYGRgYGBoYGlsZuBoTJQiABmwJ9c</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PRODUCTION OF LITHIUM PHOSPHOTITANATE SINTERED BODY</title><source>esp@cenet</source><creator>TABUCHI MITSUHARU ; TAKEUCHI TOMONARI ; ATO KAZUAKI ; KAGEYAMA HIROYUKI</creator><creatorcontrib>TABUCHI MITSUHARU ; TAKEUCHI TOMONARI ; ATO KAZUAKI ; KAGEYAMA HIROYUKI</creatorcontrib><description>PROBLEM TO BE SOLVED: To obtain a high lithium ion conductive inorganic solid electrolyte in a short-time single stage at a low temperature by supplying a DC pulsating current to a powdery mixture of an Li feed source, a Ti feed source and a P feed source under pressure. SOLUTION: As a Li feed source is exemplified, e.g. LiOH, LiOH.H2O, Li2CO3 or LiNO3. As a Ti feed source is exemplified, e.g. H2TiO3, TiO2 or Ti(SO4)2. As a P feed source is, e.g. H3PO4, Li3PO4 or H3PO2. The molar ratio among the Li, Ti and P feed sources is preferably about (5-20):(10-30):(25-45). A powdery starting material mixture is prepared by mixing and agitating the powdery Li, Ti and P feed sources in an aqueous medium. An about 200-500A DC pulsating current is supplied to the mixture under about 5-40 MPa pressure and the mixture is brought into solid phase reaction at about 250-1,000 deg.C for about 2-10 min.</description><edition>7</edition><language>eng</language><subject>ARTIFICIAL STONE ; BASIC ELECTRIC ELEMENTS ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; ELECTRICITY ; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC ; GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS ; LIME, MAGNESIA ; METALLURGY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY ; REFRACTORIES ; SLAG ; TECHNICAL SUBJECTS COVERED BY FORMER USPC ; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS ; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ARTCOLLECTIONS [XRACs] AND DIGESTS ; TREATMENT OF NATURAL STONE</subject><creationdate>2000</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20000418&amp;DB=EPODOC&amp;CC=JP&amp;NR=2000109360A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20000418&amp;DB=EPODOC&amp;CC=JP&amp;NR=2000109360A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TABUCHI MITSUHARU</creatorcontrib><creatorcontrib>TAKEUCHI TOMONARI</creatorcontrib><creatorcontrib>ATO KAZUAKI</creatorcontrib><creatorcontrib>KAGEYAMA HIROYUKI</creatorcontrib><title>PRODUCTION OF LITHIUM PHOSPHOTITANATE SINTERED BODY</title><description>PROBLEM TO BE SOLVED: To obtain a high lithium ion conductive inorganic solid electrolyte in a short-time single stage at a low temperature by supplying a DC pulsating current to a powdery mixture of an Li feed source, a Ti feed source and a P feed source under pressure. SOLUTION: As a Li feed source is exemplified, e.g. LiOH, LiOH.H2O, Li2CO3 or LiNO3. As a Ti feed source is exemplified, e.g. H2TiO3, TiO2 or Ti(SO4)2. As a P feed source is, e.g. H3PO4, Li3PO4 or H3PO2. The molar ratio among the Li, Ti and P feed sources is preferably about (5-20):(10-30):(25-45). A powdery starting material mixture is prepared by mixing and agitating the powdery Li, Ti and P feed sources in an aqueous medium. An about 200-500A DC pulsating current is supplied to the mixture under about 5-40 MPa pressure and the mixture is brought into solid phase reaction at about 250-1,000 deg.C for about 2-10 min.</description><subject>ARTIFICIAL STONE</subject><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>ELECTRICITY</subject><subject>GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC</subject><subject>GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TECHNICAL SUBJECTS COVERED BY FORMER USPC</subject><subject>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS</subject><subject>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ARTCOLLECTIONS [XRACs] AND DIGESTS</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2000</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDAOCPJ3CXUO8fT3U_B3U_DxDPHwDPVVCPDwDwbiEM8QRz_HEFeFYE-_ENcgVxcFJ3-XSB4G1rTEnOJUXijNzaDk5hri7KGbWpAfn1pckJicmpdaEu8VYGRgYGBoYGlsZuBoTJQiABmwJ9c</recordid><startdate>20000418</startdate><enddate>20000418</enddate><creator>TABUCHI MITSUHARU</creator><creator>TAKEUCHI TOMONARI</creator><creator>ATO KAZUAKI</creator><creator>KAGEYAMA HIROYUKI</creator><scope>EVB</scope></search><sort><creationdate>20000418</creationdate><title>PRODUCTION OF LITHIUM PHOSPHOTITANATE SINTERED BODY</title><author>TABUCHI MITSUHARU ; TAKEUCHI TOMONARI ; ATO KAZUAKI ; KAGEYAMA HIROYUKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2000109360A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2000</creationdate><topic>ARTIFICIAL STONE</topic><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>ELECTRICITY</topic><topic>GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC</topic><topic>GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TECHNICAL SUBJECTS COVERED BY FORMER USPC</topic><topic>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS</topic><topic>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ARTCOLLECTIONS [XRACs] AND DIGESTS</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>TABUCHI MITSUHARU</creatorcontrib><creatorcontrib>TAKEUCHI TOMONARI</creatorcontrib><creatorcontrib>ATO KAZUAKI</creatorcontrib><creatorcontrib>KAGEYAMA HIROYUKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TABUCHI MITSUHARU</au><au>TAKEUCHI TOMONARI</au><au>ATO KAZUAKI</au><au>KAGEYAMA HIROYUKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PRODUCTION OF LITHIUM PHOSPHOTITANATE SINTERED BODY</title><date>2000-04-18</date><risdate>2000</risdate><abstract>PROBLEM TO BE SOLVED: To obtain a high lithium ion conductive inorganic solid electrolyte in a short-time single stage at a low temperature by supplying a DC pulsating current to a powdery mixture of an Li feed source, a Ti feed source and a P feed source under pressure. SOLUTION: As a Li feed source is exemplified, e.g. LiOH, LiOH.H2O, Li2CO3 or LiNO3. As a Ti feed source is exemplified, e.g. H2TiO3, TiO2 or Ti(SO4)2. As a P feed source is, e.g. H3PO4, Li3PO4 or H3PO2. The molar ratio among the Li, Ti and P feed sources is preferably about (5-20):(10-30):(25-45). A powdery starting material mixture is prepared by mixing and agitating the powdery Li, Ti and P feed sources in an aqueous medium. An about 200-500A DC pulsating current is supplied to the mixture under about 5-40 MPa pressure and the mixture is brought into solid phase reaction at about 250-1,000 deg.C for about 2-10 min.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2000109360A
source esp@cenet
subjects ARTIFICIAL STONE
BASIC ELECTRIC ELEMENTS
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
ELECTRICITY
GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC
GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS
LIME, MAGNESIA
METALLURGY
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
REFRACTORIES
SLAG
TECHNICAL SUBJECTS COVERED BY FORMER USPC
TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ARTCOLLECTIONS [XRACs] AND DIGESTS
TREATMENT OF NATURAL STONE
title PRODUCTION OF LITHIUM PHOSPHOTITANATE SINTERED BODY
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-02T20%3A56%3A28IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TABUCHI%20MITSUHARU&rft.date=2000-04-18&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2000109360A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true