PRODUCTION OF TANTALUM CARBIDE

PROBLEM TO BE SOLVED: To produce low oxygen and low free carbon high-quality tantalum carbide in a good yield. SOLUTION: Tantalum oxide is mixed with carbon and primary carbonization is carried out at a prescribed temp., preferably 1,400-1,800 deg.C in a hydrogen furnace. The amts. of oxygen and fre...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SUGIMOTO TSUKASA, ISAKA HIROMICHI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To produce low oxygen and low free carbon high-quality tantalum carbide in a good yield. SOLUTION: Tantalum oxide is mixed with carbon and primary carbonization is carried out at a prescribed temp., preferably 1,400-1,800 deg.C in a hydrogen furnace. The amts. of oxygen and free carbon in the resultant carbide are measured, carbon is added to the primary carbide by an amt. adjusted on the basis of the measurements and secondary carbonization is carried out at a prescribed temp., preferably 1,800-2,000 deg.C in a vacuum carbonization furnace.