RESINE POLIESTERE AVENTI MIGLIORATE PROPRIETA
Polyster resins, particularly suitable for extrusion blow-molding, contain from 20 to 1000 ppm of a dianhydride of an aromatic tetracarboxylic acid and show values of die swell less than 45%. The resins are obtained by solid state polycondensation of resin having intrinsic viscosity less than 0.7 dl...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | ita |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Polyster resins, particularly suitable for extrusion blow-molding, contain from 20 to 1000 ppm of a dianhydride of an aromatic tetracarboxylic acid and show values of die swell less than 45%. The resins are obtained by solid state polycondensation of resin having intrinsic viscosity less than 0.7 dl/g, added with a dianhydride of an aromatic tetracarboxylic acid in amount from 0.002 and 0.1 % by weight. |
---|