PROCESSO PER LA PRODUZIONE DI OSSIDO DI CALCIO, OSSIDO DI STRONZIO ED OSSIDO DI BARIO AD ELEVATA VELOCITA' DI ASSORBIMENTO DI ACQUA ED
A process for preparing calcium oxide, strontium oxide or barium oxide consists in the treatment of the corresponding hydroxides following the reactions (I): Ca(OH)2 } CaO + H2O; (II): Sr(OH)2 } SrO + H2O; (III): Ba(OH)2 } BaO + H2O; at temperatures comprised between 400 and 900 DEG C during a time...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | ita |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A process for preparing calcium oxide, strontium oxide or barium oxide consists in the treatment of the corresponding hydroxides following the reactions (I): Ca(OH)2 } CaO + H2O; (II): Sr(OH)2 } SrO + H2O; (III): Ba(OH)2 } BaO + H2O; at temperatures comprised between 400 and 900 DEG C during a time between 1 and 15 hours under vacuum or in an inert gas atmosphere. Preferably said reaction is caused to take place in a capsule with at least a portion of surface being permeable to the gas flow. |
---|