Pharmaceutically active L-cysteine derivs
The coating material comprises filler made of 60-80% metal oxides or metal carbonates of 20 microns grain size and 40-20 w/w% hardening synthetic resin. The mixt. is finely ground to below 20 micron dia., and the homogeneous powder is dispersed in an organic solvent. @(-pp Dwg.No.0/0)
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; ita |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The coating material comprises filler made of 60-80% metal oxides or metal carbonates of 20 microns grain size and 40-20 w/w% hardening synthetic resin. The mixt. is finely ground to below 20 micron dia., and the homogeneous powder is dispersed in an organic solvent. @(-pp Dwg.No.0/0) |
---|