PROCESS FOR PRODUCING ACTIVE SINTERING ADDITIVE AND ALUMINIUM OXIDE BASIC MATERIAL FOR CERAMIC PURPOSES, COMPRISING SUCH ADDITIVE

Ca-anorthite, Ba-anorthite and Mg-silicate are ground together in ratio between 3:1:1 and 1:1:3, the mix is then burned at 1050-1280 deg.C and the cooled frit is ground and mixed with Al2O3. - The final composition comprises (%): 94-98 Al2O3, 0.1-0.6 CaO, 0.1-0.8 BaO, 0.2-0.9 MgO and 0.9-3.4 SiO2

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: PODHORANYI,GYULANE,HU, DECSI,ZOLTAN,HU, KAPTAY,GYOERGY,HU, PENZES,IMRE,HU, BORVENDEG,JOZSEF,HU, PIRIK,SANDOR,HU, FEJER,ZSOLT,HU, SZTANKOVICS,LASZLO,HU, CSIGE,JANOS,HU, SCHLEGEL,MIKLOS,HU, CSASZAR,CSABA,HU, TOTH,BENJAMINNE,HU, TOTH,IMRE,HU
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Ca-anorthite, Ba-anorthite and Mg-silicate are ground together in ratio between 3:1:1 and 1:1:3, the mix is then burned at 1050-1280 deg.C and the cooled frit is ground and mixed with Al2O3. - The final composition comprises (%): 94-98 Al2O3, 0.1-0.6 CaO, 0.1-0.8 BaO, 0.2-0.9 MgO and 0.9-3.4 SiO2