PROCESS AND FURNACE FOR PREPARING ALUMINA

A suspension of Al(OH)3 is dried and then ignited. Part (0.5-5 kg/kg) of the ignited Al2O3 is returned to the dehydration stage, where the density of the vortex layer is kept at 300-900 kg/m3. The furnace consists of a cyclonic heat exchanger for drying, a shaft furnace for dehydration and an igniti...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TELJATNYIKOV,GARRY V,SU, KARPOV,ANATOLIJ B,SU, SZTYAZKIN,ANATOLIJ K,SU, SZOKOLOV,PAVEL I,SU, LJAKOV,VIKTOR P,SU, USZTYINOV,VLAGYIMIR K,SU, PINJUGIN,JURIJ V,SU, SMORGUNYENKO,NYIKOLAJ SZ,SU, SAMULJOV,BORISZ L,SU, GORSKOV,NYIKOLAJ I,SU, SZMIRNOV,VADIM SZ,SU, GONCSAROV,VITALIJ K,SU, BLINKIN,KONSTANTIN G,SU, FOMIN,EDUARD SZ,SU, MILRUD,SZAVELJ M,SU, ARLJUK,TAMARA A,SU, KAIM,GERMAN A,SU
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A suspension of Al(OH)3 is dried and then ignited. Part (0.5-5 kg/kg) of the ignited Al2O3 is returned to the dehydration stage, where the density of the vortex layer is kept at 300-900 kg/m3. The furnace consists of a cyclonic heat exchanger for drying, a shaft furnace for dehydration and an ignition chamber, which is divided in two parts with different grating.