Improvements in or relating to a copper-based alloy
A copper alloy containing between 0.001 and 0.05% by weight of tellurium and between 0.001 and 0.01% by weight of phosphorus is manufactured by forming a molten mass of the alloy and casting the molten mass in such a way that it solidifies rapidly at a speed greater than 1.5 mm per second, with a hi...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A copper alloy containing between 0.001 and 0.05% by weight of tellurium and between 0.001 and 0.01% by weight of phosphorus is manufactured by forming a molten mass of the alloy and casting the molten mass in such a way that it solidifies rapidly at a speed greater than 1.5 mm per second, with a high cooling rate, greater than 20 DEG C per second through the entire thickness of the cast mass. |
---|