PROCEDE DE PRODUCTION D'UNE FEUILLE LAQUEE POUR LA DEPOSITION SUR UNE PIECE, ET SON UTILISATION

The production procedure uses a carrier layer of a sheet metal or plastic material (3) between 100 and 1200 mcm thick, with a first coat of paint, 10 - 50 mcm thick when dry, applied by scraper, roller, pouring or printing, and a second coat (9) applied by spray. The thickness of the first coat is 3...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: AICHHOLZER WALTER, GRUBER THOMAS, BERKAU REINHOLD, ROTHENBURGER HOLGER
Format: Patent
Sprache:fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The production procedure uses a carrier layer of a sheet metal or plastic material (3) between 100 and 1200 mcm thick, with a first coat of paint, 10 - 50 mcm thick when dry, applied by scraper, roller, pouring or printing, and a second coat (9) applied by spray. The thickness of the first coat is 3 - 5 times greater than that of the second coat when dry. The production procedure uses a carrier layer of a sheet metal or plastic material (3) between 100 and 1200 mcm thick, with a first coat of paint, 10 - 50 mcm thick when dry, applied by scraper, roller, pouring or printing, and a second coat (9) applied by spray. The thickness of the first coat is 3 - 5 times greater than that of the second coat when dry, and the second coat is followed by a covering layer (11) of a transparent paint that is hardened by UV rays.