Process for the preparation of a catalyst for reforming naphtha

Process comprising the operations consisting in acidifying aluminium hydroxide in a certain concentration between 60 and 250 DEG C in a vapour atmosphere for 2 to 15 hours and then forming and calcining the aluminium hydroxide formed between 450 and 700 DEG C to form a gamma-alumina support which is...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SUN FENGDUO, XU YUANGUO
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Process comprising the operations consisting in acidifying aluminium hydroxide in a certain concentration between 60 and 250 DEG C in a vapour atmosphere for 2 to 15 hours and then forming and calcining the aluminium hydroxide formed between 450 and 700 DEG C to form a gamma-alumina support which is supported by Pt, Re and Ti and by halogen, the contents of the said metals and of halogen being 0.075 to 0.80 of Pt, 0.075 to 1.50 of Re, 0.00 to 0.40 of Ti, and 0.50 to 2.00 of halogen, on the basis of the % by weight of dry alumina. … … La présente invention concerne un procédé pour la préparation d'un catalyseur de reformage de naphta. Procédé comprenant les opérations consistant à acidifier l'hydroxyde d'aluminium dans une certaine concentration entre 60 et 250degré C dans une atmoosphère de vapeur pendant 2 à 15 heures, puis à former, calciner l'hydroxyde d'aluminium formé entre 450 et 700degré C pour former un support d'alumine- gamma qui est supporté par Pt, Re et Ti et par l'halogène, les contenus desdits métaux et de l'halogène étant de 0,075 à 0,80 de Pt, de 0,075 à 1,50 de Re, de 0,00 à 0,40 de Ti, de 0,50 à 2,00 en halogène, sur la base du % en poids d'alumine séché.