COMPOSITION ET PROCEDE POUR PREPARER UN MATERIAU RESISTANT A L'EAU ET ISOLANT A LA CHALEUR A BASE DE SILICATE DE SODIUM LIQUIDE

A water resistant and thermally insulating silicate article is produced using a starting mixture having the oxidic composition: from 62 to 68% SiO2; from 1.5 to 5% Al2O3; from 5 to 10% B2O3; from 0.1 to 0.5% CaO+MgO and from 21 to 26% by weight Na2O, all percentages being expressed on a weight basis...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: MARIN ALEXANDROV POPOV, TODOR GEORGIEV GEORGIEV, BOGDAN BORISSOV KLISURSKI ET GEORGI GEORGIEV MALINOV
Format: Patent
Sprache:fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A water resistant and thermally insulating silicate article is produced using a starting mixture having the oxidic composition: from 62 to 68% SiO2; from 1.5 to 5% Al2O3; from 5 to 10% B2O3; from 0.1 to 0.5% CaO+MgO and from 21 to 26% by weight Na2O, all percentages being expressed on a weight basis, and subjecting the mixture to baking at a temperature of 600 to 700 DEG C. The oxidic composition is suitably provided by a mixture of liquid and solid sodium silicate, borax and perlite.