Formulaciones adhesivas de los polímeros (S-I/B)X radiales
The invention relates to an adhesive composition comprising (i) one or more styrenic block copolymer compositions, (ii) a tackifier resin, and (iii) one or more plasticizers, wherein said styrenic block copolymer composition comprises: a. a tetra-branched block copolymer (IV) represented by the gene...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | spa |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention relates to an adhesive composition comprising (i) one or more styrenic block copolymer compositions, (ii) a tackifier resin, and (iii) one or more plasticizers, wherein said styrenic block copolymer composition comprises: a. a tetra-branched block copolymer (IV) represented by the general formula (A-B)4X; b. a tri-branched block copolymer (III) represented by the general formula (A-B)3X; c. a di-branched block copolymer (II) represented by the general formula (A-B)2X; and d. a linear diblock copolymer (I) represented by the general formula A-B; where: i. A represents a polymer block of a mono alkenyl arene; ii. B represents a polymer block of a mixture of isoprene and 1,3-butadiene in a weight ratio of isoprene to butadiene from about 70:30 to about 40:60; iii. X represents the residue of a multi-functional coupling agent; iv. the weight percent of A blocks is from about 14% to about 22%; v. the relative amounts of copolymers IV, III, II, and I are from 0 to 20 weight percent IV, from 50 to 80 weight percent III, from 0 to 20 weight percent II and from 20 to 50 weight percent I, where the total of I, II, III and IV equals 100 weight percent; and vi. the melt flow rate of the polymer composition is at least 2.0 g/10 minutes at 200° C./5 kg as measured by ASTM D1238 (D condition). |
---|