Gold leaching
Leaching of gold-bearing solids, such as crushed lean ores or material recovered from very old waste tips can be carried out with a dilute aqueous alkali cyanide solution, but the extent and/or rate of recovery of gold is impaired by the anaerobic or reducing conditions that can exist in such heaps,...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; spa |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Leaching of gold-bearing solids, such as crushed lean ores or material recovered from very old waste tips can be carried out with a dilute aqueous alkali cyanide solution, but the extent and/or rate of recovery of gold is impaired by the anaerobic or reducing conditions that can exist in such heaps, and especially towards their base and or by poor supply of oxygen in agitation leaching. The rate and/or extent of gold recovery in heap leaching can be increased and the supply of oxygen simply controlled by slow release in agitation leaching, using otherwise identical conditions by employing an effective amount of a slow dissolving poorly soluble solid metal peroxide, either by incorporating it within the heap or in the mixture of gold-bearing solids and lixiviant. The peroxide is advantageously calcium peroxide because it is not only very effective but also is environmentally suitable. The amount employed is preferably from 1 to 10 parts w/w per 1000 parts of gold-bearing solids for the low grade material, usually containing from 1 to 10 g gold per tonne solids.
UN PROCEDIMIENTO PARA LA EXTRACCION DE ORO DE MATERIALES SOLIDOS QUE LO CONTIENEN. LA LIXIVIACION DE SOLIDOS AURIFEROS, TALES COMO MINERALES POBRES TRITURADOS O MATERIALES RECUPERADOS DE RESIDUOS MUY VIEJOS, SE PUEDE EFECTUAR CON UNA SOLUCION ACUOSA DILUIDA DE UN CIANURO ALCALINO, PERO EL GRADO Y/O LA VELOCIDAD DE RECUPERACION DEL ORO SE VE PERJUDICADA POR LAS CONDICIONES ANAEROBICAS O REDUCTORAS QUE PUEDEN EXISTIR EN ESOS MONTONES, ESPECIALMENTE EN LA BASE Y SUS PROXIMIDADES, Y/O POR EL ESCASO SUMINISTRO DE OXIGENO EN LA LIXIVIACION POR AGITACION. LA VELOCIDAD Y/O EL GRADO DE RECUPERACION DE ORO EN LA LIXIVIACION DE MONTONES PUEDE INCREMENTARSE Y EL SUMINISTRO DE OXIGENO PUEDE CONTROLARSE SENCILLAMENTE MEDIANTE LA LIBERACION LENTA EN LA LIXIVIACION POR AGITACION, MANTENIMIENTO POR LO DEMAS CONDICIONES IDENTICAS, EMPLEANDO UNA CANTIDAD EFICAZ DE UN PEROXIDO METALICO SOLIDO POCO SOLUBLE, QUE SE DISUELVA LENTAMENTE, YA SEA INCORPORANDOLO DENTRO DEL MONTON O EN LA MEZCLA DE SOLIDOS AURIFEROS YLIXIVIANTE. VENTAJOSAMENTE, EL PEROXIDO ES PEROXIDO DE CALCIO YA QUE, NO SOLO ES MUY EFICAZ, SINO QUE ADEMAS ES ADECUADO DESDE EL PUNTO DE VISTA MEDIOAMBIENTAL. PREFERIBLEMENTE LA CANTIDAD EMPLEADA ES DE 1 A 10 PARTES EN PESO POR CADA 1.000 PARTES DE SOLIDOS AURIFEROS PARA EL MATERIAL DE BAJA CALIDAD, QUE CONTIENE NORMALMENTE DE 1 A 10 G DE ORO POR TONELADA DE SOLIDOS. |
---|