COMPOSITE POSITIVE ELECTRODE MATERIAL, AND PREPARATION METHOD THEREFOR AND USE THEREOF
A composite positive-electrode material includes LMFP and LFP. The LMFP has a primary particle size in a range of 20nm-200 nm. The LFP has a primary particle size in at least two ranges of: 100nm-200 nm; 200nm-350 nm; 350nm-500 nm; and 500nm-1000 nm. The primary particle size of the LFP is larger th...
Gespeichert in:
Hauptverfasser: | , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A composite positive-electrode material includes LMFP and LFP. The LMFP has a primary particle size in a range of 20nm-200 nm. The LFP has a primary particle size in at least two ranges of: 100nm-200 nm; 200nm-350 nm; 350nm-500 nm; and 500nm-1000 nm. The primary particle size of the LFP is larger than the primary particle size of the LMFP. |
---|