METHOD FOR PREPARING A MIXTURE OF RAW MATERIALS COMPRISING CALCIUM OXIDE
Method for manufacturing glass, comprising preparing a mixture of glass raw materials for a glassworks furnace, wherein water, sand and sodium carbonate are mixed in mass proportions of between 0 and 5%, 40 and 65%, and more than 0 and no more than 25% respectively, and, within a time of less than 1...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Method for manufacturing glass, comprising preparing a mixture of glass raw materials for a glassworks furnace, wherein water, sand and sodium carbonate are mixed in mass proportions of between 0 and 5%, 40 and 65%, and more than 0 and no more than 25% respectively, and, within a time of less than 10 minutes, preferably simultaneously, calcium oxide is added in a mass proportion of between 1 and 20% of the total, the calcium oxide has a granulometry such that more than 97% by mass does not pass through a sieve of 0.125 mm, more than 96% by mass does not pass through a sieve of 0.5 mm, preferably more than 95% by mass does not pass through a sieve of 1 mm. |
---|