AQUEOUS WATER BARRIER COATINGS
Described herein is a multi-phase polymer binder comprising:an aqueous polymer dispersion present in an amount of 65 wt% to 100 wt%;a hydrophobic emulsion from 0 wt% to 25 wt%; anda surfactant from 0 wt% to 10 wt%;wherein the polymer binder, when dried, provides a water uptake of less than 5 g/m2/20...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Described herein is a multi-phase polymer binder comprising:an aqueous polymer dispersion present in an amount of 65 wt% to 100 wt%;a hydrophobic emulsion from 0 wt% to 25 wt%; anda surfactant from 0 wt% to 10 wt%;wherein the polymer binder, when dried, provides a water uptake of less than 5 g/m2/20 min in accordance with Cobb test, a seal strength of at least 200 Newton/meter (N/m) as measured at 25 °C and 90 °C, and block resistance of 3 to 5 when measured at 50° C and 60 psi for 24 hours in accordance with the method described in the description, andthe aqueous polymer dispersion comprises an acid-rich copolymer present in an amount of 5 wt% to 60 wt%; and an acid-free copolymer present in an amount of 40 wt% to 95 wt%, wherein the acid-rich copolymer comprises carboxylic acid functional monomers in an amount of 5 wt% to 25 wt%; styrene in an amount of up to 70 wt%; and (meth)acrylate monomers in an amount of 10 wt% to 90 wt%, andthe acid-free copolymer comprises styrene in an amount of up to 50 wt%; and (meth)acrylate monomers in an amount of 50 wt% to less than 100 wt%, andwherein the aqueous polymer dispersion has a solids content (NV %) from 40.3 to 47.9%. |
---|