Disclosed are a steel board for polar marine engineering and a preparation method therefor. According to weight percentage, the components of the steel board are: C: 0.06-0.09%, Si: 0.20-0.35%, Mn: 1.48-1.63%, Nb: 0.020%-0.035%, Ti: 0.010%-0.020%, V: 0.020%-0.035%, Ni: 0.08%-0.17%, Als: 0.015%-0.040...
Gespeichert in:
Hauptverfasser: | , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Disclosed are a steel board for polar marine engineering and a preparation method therefor. According to weight percentage, the components of the steel board are: C: 0.06-0.09%, Si: 0.20-0.35%, Mn: 1.48-1.63%, Nb: 0.020%-0.035%, Ti: 0.010%-0.020%, V: 0.020%-0.035%, Ni: 0.08%-0.17%, Als: 0.015%-0.040%, P: ≤ 0.013% and S: ≤ 0.005%. The preparation method for the steel board comprises: pre-refining, refining and casting to obtain a cast billet, and the slowly cooling down same. The slowly cooled billet is heated and then rolled out to obtain the steel board; and the steel board is cooled down and ready. The steel has an excellent comprehensive performance in terms of having high strength and low temperature resistance, being easy to weld and corrosion proof, and the steel has good low-temperature aging impact toughness. |
---|