METHOD FOR RECRYSTALLISATION ANNEALING OF A NON-GRAIN-ORIENTED ELECTRIC STRIP

A method for the recrystallisation annealing of a non-grain-oriented electric strip (2) in a continuous annealing and coating line (1) is presented. Therein, the electric strip (2) is heated in an induction furnace (5) to a temperature of at least 680° C. at a heating rate of at least 80 K/s and the...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HALLEUX, Pierre-Yves, BÖTTCHER, Andreas, MASCHLER, Frank
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A method for the recrystallisation annealing of a non-grain-oriented electric strip (2) in a continuous annealing and coating line (1) is presented. Therein, the electric strip (2) is heated in an induction furnace (5) to a temperature of at least 680° C. at a heating rate of at least 80 K/s and then, in an optional second continuous furnace (8), to a temperature of at least 820° C. at a heating rate of at most 20 K/s. The electric strip (2) is initially heated before the induction furnace (5) via a first continuous furnace (3) to a temperature of at least 300° C. at a heating rate of at most 60 K/s.