NEODYMIUM-IRON-BORON MAGNET MATERIAL, RAW MATERIAL COMPOSITION, PREPARATION METHOD THEREFOR AND USE THEREOF
Disclosed are a neodymium-iron-boron magnet material, a raw material composition, a preparation method therefor and a use thereof. The raw material composition of the neodymium-iron-boron magnet material comprises the following components in weight content: R: 28-33%; R being rare earth elements, an...
Gespeichert in:
Hauptverfasser: | , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Disclosed are a neodymium-iron-boron magnet material, a raw material composition, a preparation method therefor and a use thereof. The raw material composition of the neodymium-iron-boron magnet material comprises the following components in weight content: R: 28-33%; R being rare earth elements, and comprising R1 and R2, R1 being a rare earth element added during smelting, R1 comprising Nd and Dy, R2 being a rare earth element added during grain boundary diffusion, R2 comprising Tb, and the content of R2 being 0.2-1%; M: ≤0.4% but not 0, M being one or more elements among Bi, Sn, Zn, Ga, In, Au and Pb; Cu: ≤0.15% but not 0; B: 0.9-1.1%; Fe: 60-70%; but not containing Co. The neodymium-iron-boron magnet material under the condition of adding a small amount of heavy rare earth elements and not adding cobalt, can still have a relatively high coercivity and remanence, and excellent thermal stability. |
---|