SYNTHETIC GRAPHITE MATERIAL, SYNTHETIC GRAPHITE MATERIAL PRODUCTION METHOD, NEGATIVE ELECTRODE FOR LITHIUM ION SECONDARY BATTERY, AND LITHIUM ION SECONDARY BATTERY
Provided is a synthetic graphite material, in which a size L (112) of a crystallite in a c-axis direction as calculated from a (112) diffraction line obtained by an X-ray wide angle diffraction method is in a range of 4 to 30 nm, a surface area based on a volume as calculated by a laser diffraction...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Provided is a synthetic graphite material, in which a size L (112) of a crystallite in a c-axis direction as calculated from a (112) diffraction line obtained by an X-ray wide angle diffraction method is in a range of 4 to 30 nm, a surface area based on a volume as calculated by a laser diffraction type particle size distribution measuring device is in a range of 0.22 to 1.70 m2/cm3, an oil absorption is in a range of 67 to 147 mL/100 g, and a nitrogen adsorption specific surface area is in a range of 3.1 to 8.2 m2/g. |
---|