REINFORCED POLYESTER STRUCTURAL COMPONENTS

An article of manufacture comprising a polyester composition, the article comprising, as measured by differential scanning calorimetry with a heating rate of 20° C. per minute on first heating according to ASTM D3418, at least two different crystalline melting temperatures, wherein a first crystalli...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: COLLAR, Curtis, GALLUCCI, Robert Russell, DAGA, Vikram K, MUNJURULIMANA, Dinesh, CHANG, Fred, FAKIRI, Abderrahim
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:An article of manufacture comprising a polyester composition, the article comprising, as measured by differential scanning calorimetry with a heating rate of 20° C. per minute on first heating according to ASTM D3418, at least two different crystalline melting temperatures, wherein a first crystalline melting temperature and a second crystalline melting temperature are each independently 200-290° C.; and a first heat of fusion and a second heat of fusion that are each independently at least 3 J/g, preferably wherein a ratio of the first heat of fusion to the second heat of fusion is 1:5-5:1, wherein the polyester composition comprises a first polyester having a phosphorous content of greater than or equal to 20 ppm, a second polyester, and 5-50 weight percent of a plurality of fibers, based on the total weight of the polyester composition, wherein the plurality of fibers have a diameter of 5-25 micrometers.