FIBER PRODUCTION METHOD AND CARBON FIBER PRODUCTION METHOD
A method of producing a fiber, the method including discharge, from a spinneret 1, a spinning dope solution containing a fiber-forming polymer dissolved in a solvent, once allowing the solution to run in air, and then guiding the solution into the liquid of a coagulation bath 4 to allow coagulation,...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A method of producing a fiber, the method including discharge, from a spinneret 1, a spinning dope solution containing a fiber-forming polymer dissolved in a solvent, once allowing the solution to run in air, and then guiding the solution into the liquid of a coagulation bath 4 to allow coagulation, wherein a gas-phase portion formed in a vertically downward direction from a discharge surface of the spinneret 1 to the liquid surface of the coagulation bath 4 has an air flow rate per unit time (Af) which satisfies, in relation to the amount of the solvent in the spinning dope solution per unit time (As) in the gas-phase-portion volume (Vh), the relational expression 0.0008 m3 ≤ Af/(As/Vh) ≤ 0.0015 m3, and the hourly average of the absolute humidity at each of four points in an outer periphery of the spinneret in the gas-phase portion is not more than 20 g/m3.A method of producing a fiber, which, in dry-jet wet spinning, suppresses occurrence of dew condensation in the spinneret, and reduces deterioration of the appearance caused by winding on rollers in the subsequent process or by fuzzing or yarn break in the stretching process, to enable significant improvement of the productivity and the appearance as a whole, is provided. |
---|