SORBENTS FROM IRON-RICH AND ALUMINIUM-RICH STARTING MATERIALS

Method of manufacturing a sorbent material, comprising mixing (11) a first granular material (20) comprising iron and a second granular material (30) comprising aluminium hydroxide to obtain a mixture. The mixture is subjected to a thermal treatment (12) at a temperature between 400°C and 950°C.

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: JENNÉ, Rika, PELEMAN, Gisèle, BERGMANS, Jef, MICHIELSEN, Bart, BROOS, Kris
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Method of manufacturing a sorbent material, comprising mixing (11) a first granular material (20) comprising iron and a second granular material (30) comprising aluminium hydroxide to obtain a mixture. The mixture is subjected to a thermal treatment (12) at a temperature between 400°C and 950°C.